This work studied the performance of Ni-based catalysts derived from LaNiO3 and CeSiO2 supported LaNiO3 perovskite-type oxides for the steam reforming of ethanol. In situ XRD and TPR revealed the presence of different Ni species on both calcined samples: LaNiO3, La2NiO4 and NiO phases. Both catalysts deactivated during the reaction. Ni sintering was ruled out based on the in situ XRD experiments under reaction conditions. For LaNiO3, metallic Ni particles were partially oxidized by the water present in the feed at the beginning of the reaction. Then, NiO particles formed were reduced again by the syngas produced during the reaction. TG analysis showed significant carbon formation on LaNiO3 catalyst. However, carbon formation was significantly decreased over LaNiO3/CeSiO2 catalyst, which was due to the important role of the support on the mechanism of carbon removal for steam reforming of ethanol. (C) 2016 Elsevier B.V. All rights reserved.
机译:这项工作研究了由LaNiO3和CeSiO2负载的LaNiO3钙钛矿型氧化物衍生的镍基催化剂在乙醇蒸汽重整方面的性能。原位XRD和TPR显示两种煅烧样品上均存在不同的Ni物种:LaNiO3,La2NiO4和NiO相。反应期间两种催化剂均失活。基于反应条件下的原位XRD实验,排除了Ni烧结。对于LaNiO3,金属Ni颗粒在反应开始时就被进料中存在的水部分氧化。然后,形成的NiO颗粒被反应过程中产生的合成气再次还原。 TG分析显示在LaNiO 3催化剂上明显的碳形成。但是,相比于LaNiO3 / CeSiO2催化剂,碳的形成明显减少,这是由于载体对乙醇蒸汽重整的碳去除机理的重要作用。 (C)2016 Elsevier B.V.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号