Hydrothermal doping method for preparation of Cr~(3+)-TiO_2 photocatalysts with concentration gradient distribution of Cr~(3+)

机译:水热掺杂法制备Cr〜(3+)浓度梯度分布的Cr〜(3 +)-TiO_2光催化剂

获取原文
获取原文并翻译 | 示例
           

摘要

Cr~(3+)-doped anatase titanium dioxide photocatalysts were prepared by the combination of sol-gel process with hydrothermal treatment.The samples were characterized by UV-vis diffuse reflectance spectroscopy,X-ray diffraction (XRD),Brunauer-Emmett-Teller (BET) specific surface area (SBETX transmission electron microscopy (TEM),atomic absorption flame emission spectroscopy (AAS),electron paramagnetic resonance (EPR) spectroscopy and X-ray photoelectron spectroscopy (XPS).It was confirmed that Cr substitutes Ti~(4+) in TiO_2 lattice in trivalent ionic state,and the concentrations of dopants Cr~(3+) decrease from the exterior to the interior of doped TiO_2.The photocatalytic activity of Cr-TiO_2 was investigated for the photocatalytic degradation of XRG aqueous solution both under UV and visible light irradiation.Due to the excitation of 3d electron of Cr~(3+) to the conduction band of TiO_2,Cr-TiO_2 shows a good ability for absorbing the visible light to degrade XRG.Doping of chromium ions effectively improves the photocatalytic activity under both UV light irradiation and visible light irradiation with an optimal doping concentration of 0.15% and 0.2%,respectively.The special distribution of dopants Cr~(3+) seems having a good effect on enhancing the photocatalytic activity of Cr-TiO_2.
机译:溶胶-凝胶法与水热处理相结合制备了Cr〜(3+)掺杂的锐钛矿型二氧化钛光催化剂。采用紫外可见漫反射光谱,X射线衍射(XRD),Brunauer-Emmett-柜员(BET)比表面积(SBETX透射电子显微镜(TEM),原子吸收火焰发射光谱(AAS),电子顺磁共振(EPR)光谱和X射线光电子能谱(XPS)。证实了Cr替代了Ti〜三价离子态的TiO_2晶格中的(4+),掺杂剂Cr〜(3+)的浓度从掺杂的TiO_2的外部到内部降低。研究了Cr-TiO_2的光催化活性对XRG水溶液的光催化降解Cr〜(3+)的3d电子被激发到TiO_2的导带上,Cr-TiO_2表现出良好的吸收可见光降解XRG的能力。 ns分别以0.15%和0.2%的最佳掺杂浓度有效地改善了在紫外光照射和可见光照射下的光催化活性。掺杂剂Cr〜(3+)的特殊分布似乎对增强光催化活性具有良好的作用。 Cr-TiO_2。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号