The K2Ti6-xZrxO13 (x = 0-1) solid solution was prepared by the traditional solid-state synthesis method. The X Ray diffraction patterns presented a proportional increase in the cell volume and crystal lattice distortion according to the increment of the Zr4+ species concentration in the reactant mixture. The morphological characterization showed a decrease in particle size average as a result of the zirconium presence due to crystal distortion. The photocatalytic performance was evaluated in the hydrogen evolution reaction in the presence of methanol. In this context, the K2Ti5ZrO13 solid solution exhibited the highest performance (72 mu molg(-1) h(-1)) due to the higher presence of defects such as oxygen vacancies because of the Zr incorporation into the crystalline structure. In this context, these anionic defects can act as electron traps in bulk material and reduce recombination of charges; meanwhile, oxygen vacancies in surface create reactive Ti3+ ions, where the reactions of interest take place.
机译:采用传统的固相合成方法制备了K2Ti6-xZrxO13(x=0-1)固溶体。X射线衍射图显示,随着反应物混合物中Zr4+物种浓度的增加,晶胞体积和晶格畸变成比例增加。形态表征表明,由于晶体变形,锆的存在导致平均粒径减小。在甲醇存在下的析氢反应中评估了光催化性能。在这种情况下,K2Ti5ZrO13固溶体表现出最高的性能(72μmolg(-1)h(-1)),这是因为Zr掺入晶体结构后,更容易出现氧空位等缺陷。在这种情况下,这些阴离子缺陷可以在大块材料中充当电子陷阱,减少电荷的复合;同时,表面的氧空位会产生活性Ti3+离子,在那里发生感兴趣的反应。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号