Composition Region of Homogeneous Liquid Phase in Lead-Containing Slags Related to QSL Process

机译:与QSL工艺相关的含铅渣中均相液相的组成区域

获取原文
获取原文并翻译 | 示例
           

摘要

As a fundamental study to control compositions ofthe slag in the oxidation zone of a QSL lead smelting furnace,phase equilibrium between the metallic lead and the PbO-FeOx-CaO-SiO2 or PbO-FeOx-CaO-SiO2-ZnO slag was investigated at1,323~1,523K and a composition region of the homogeneousliquid slag phase and the composition and chemical formula ofsolid phases in the slag coexisting with the liquid phase weredetermined. The PbO-FeOx-CaO-SiO2 slag with Q(=mass %CaO/(mass% CaO+mass% SiO2 )) of 0.4 is completely fusible at1,423K when the mole fraction ratio of FeOx, R, defined asR=NFeOx/(NFeOxNCaO+NSiO2), is around 0.4, and departure fromthis value gives rise to a solid-liquid two phase region in therange of the low PbO content.
机译:作为控制QSL铅冶炼炉的氧化区中炉渣组合物的基本研究,研究了金属铅和PbO-Feox-CaO-SiO2或PbO-Feox-CaO-SiO2-ZnO渣之间的相平衡, 323〜1,523K和均相水瓶渣相的组成区域和渣中的组合物和化学式与液相中的炉渣共存。 当Feox,R,定义的Asr = Nfeox的摩尔级分比时,具有0.4的PbO-Feox-CaO-SiO 2炉渣为0.4的Q(=质量%CaO /(质量CaO +质量%SiO 2))AT1,423K完全熔至1,423K (NfeoxncaO + NSIO2),约为0.4,并且脱离该值从低PBO含量产生固像性的固液两相区域。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号