Fine powders of lanthanum modified (Pb0.92La0.08)(Zr0.60Ti0.40) (PLZT 8/60/40) were processed by high energy mechanical ball milling. The ceramic pellets from these powders were sintered by using microwave sintering. Microwave processed ceramics were further investigated for their sintering behaviour, microstructure, dielectric and piezoelectric properties. The XRD pattern of PLZT shows a single phase formation except for the ceramics sintered at 1200 degrees C. Higher density and more uniform grain distribution were found for PLZT ceramics, microwave sintered at 1150 degrees C, in spite of having much shorter sintering time. As a result, comparable dielectric and piezoelectric properties were obtained for microwave sinterd PLZT ceramics. These show the grain size similar to 1.2 mu m, and the highest relative density similar to 99.46%. The dielectric constant for the unpoled PLZT ceramics was found to be similar to 2100. The piezoelectric charge (d(33)) and electromechanical coupling coefficient (k(p)) value for the PLZT ceramics were found to be, similar to 574 pC/N and similar to 67% respectively. (C) 2016 Elsevier Ltd. All rights reserved.
机译:通过高能机械球铣削加工镧的细粉(PB0.92LA0.08)(Zr0.60ti0.08)(Zr0.60ti0.40)(PLZT 8/60/40)。通过使用微波烧结烧结来自这些粉末的陶瓷粒料。进一步研究微波加工陶瓷,用于它们的烧结行为,微观结构,电介质和压电性能。 PLZT的XRD图案显示除陶瓷以1200℃烧结的陶瓷外,发现较高的密度和更均匀的晶粒分布,用于在1150℃下烧结微波,尽管烧结时间更短。结果,获得了可比较的电介质和压电性能,用于微波Sinterd PLZT陶瓷。这些显示与1.2μm相似的晶粒尺寸,相对于99.46%的最高相对密度。发现未浸没的PLZT陶瓷的介电常数与2100类似。发现PLZT陶瓷的压电电荷(D(33))和机电耦合系数(K(P))值,类似于574 PC / n分别与67%相似。 (c)2016 Elsevier Ltd.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号