Interlaminar shear properties of nanostitched/nanoprepreg aramid/phenolic composites by short beam method

机译:短梁法通过短梁法的纳米型/纳米吡咯族芳酰胺/酚醛复合材料的剪切性能

获取原文
获取原文并翻译 | 示例
           

摘要

The interlaminar shear strengths of nanostitched 3D aramid/phenolic composites were studied. Stitching slightly improved the interlaminar strength of the z-stitching/nanotube composites. In addition, the stitching fiber type influenced the interlaminar strength of the z-stitching/nanotube aramid/phenolic composites. The failures of all structures in the compression and tensile sides were almost negligible. However, all structures had interlaminar shear failure where delamination in z-stitching/nanotube composites was arrested. The introduction of the stitching yarn in the baseline structure improved its out-of-plane failure properties without reducing the in-plane properties. The effects of stitching and multiwall carbon nanotubes on the 3D aramid/phenolic composite were encouraging and the nanostitched para-aramid/phenolic nanocomposite could be considered as damage tolerance material.
机译:研究了纳米型3D芳族聚酰胺/酚醛复合材料的interlaInar剪切强度。 缝合略微改善Z缝合/纳米管复合材料的层间强度。 此外,缝合纤维型影响Z缝合/纳米管芳族芳酰胺/酚醛复合材料的层间强度。 压缩和拉伸侧面的所有结构的故障几乎可以忽略不计。 然而,所有结构具有层间剪切失效,其中Z缝合/纳米管复合材料中的分层被捕。 基线结构中的缝合纱线的引入改善了其外平面失效特性,而不减少面内特性。 缝合和多壁碳纳米管对3D芳族聚酰胺/酚类复合材料的影响令人鼓舞,并且纳米稳定的对芳族芳酰胺/酚醛纳米复合材料可被认为是损伤耐受材料。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号