Magnetically separable TiO2/SiO2/Fe3O4 Composites of different core (Fe3O4) diameters and silica contents have been prepared by sol-gel technique for both silica and titania coatings. Energy dispersive X-ray fluorescence (EDX), X-ray diffraction (XRD), X-ray photoelectron spectroscopy (XPS), BET surface area analysis and scanning electron microscope (SEM) have been used for characterization of prepared samples. Photocatalytic activity of the prepared samples has been investigated by photodegradation of methyl orange. Obtained results have shown that 25-45 mu m core diameter exhibits the maximum activity since it possesses a convenient surface area and light transmittance. Silica content has a significant effect on the activity of composite. Silica content of more than 10 wt% has reduced the catalyst activity because of the increase in particle diameter and reduction of surface area. (C) 2007 Elsevier Masson SAS. All rights reserved.
机译:通过溶胶 - 凝胶技术为二氧化硅和二氧化钛涂层制备不同芯(Fe3O4)直径和二氧化硅含量的磁性可分离的TiO2 / SiO2 / Fe3O4复合材料。 能量分散X射线荧光(EDX),X射线衍射(XRD),X射线光电子能谱(XPS),BET表面积分析和扫描电子显微镜(SEM)已被用于制备样品的表征。 通过光降解甲基橙,研究了制备样品的光催化活性。 获得的结果表明,25-45μm芯直径表现出最大活性,因为它具有方便的表面积和透光率。 二氧化硅含量对复合材料的活性有显着影响。 由于粒径和表面积的还原,二氧化硅含量超过10wt%降低了催化剂活性。 (c)2007年Elsevier Masson SAS。 版权所有。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号