A silicalite clay composite membrane was produced by hydrothermal deposition using tetraethyl orthosilicate (TEOS) as silica source, tetra-n-propylammonium bromide (TPABr) as template and KOH as mineralizing agent. Silicalite was deposited in the mesopores and on the surface of porous ceramic membrane supports made from a naturally available clay mineral abundantly found in the central region of Morocco (Meknès). Three flat-disc membrane supports were prepared by uniaxial pressure on pure clay powder (AS), mixture of clay and activated carbon (5%, w/w) (AC) and mixture of clay and starch (20% w/w) (AA). The porosity of membrane supports was studied as function of the final calcination temperature. It was found that the mesopores contribution to porosity was 25%, however their contribution to the specific surface area is more than 90%. The mesopores structure was investigated. XRD confirms the formation of crystalline silicalite layers inside the mesopores of the clay flat-disc supports. Typical MFI-type zeolite morphology was confirmed by SEM. The scope and limitations of the membranes in terms of selectivity between SF6and N2, is discussed.
机译:通过使用四乙基硅酸盐(TEOS)作为二氧化硅源,四丙基溴化铵(TPABR)作为模板和KOH作为矿化剂来制备硅粘土复合膜。硅沸石沉积在中孔中,并在多孔陶瓷膜支撑体上沉积在摩洛哥中部地区(Meknès)中的天然粘土矿物制成的多孔陶瓷膜支撑件。通过单轴压力在纯粘土粉末(AS)上,粘土和活性炭混合物(5%,W / W)(AC)和粘土和淀粉的混合物(20%w / w)制备三种平面膜载体AA)。研究了膜载体的孔隙率作为最终煅烧温度的函数。发现孔隙率的贡献为25%,但它们对比表面积的贡献大于90%。研究了中孔结构。 XRD确认在粘土扁平盘支撑件的中孔内的结晶硅藻土层的形成。 SEM通过SEM确认典型的MFI型沸石形态。讨论了膜在SF6和N2之间的选择性方面的范围和限制。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号