In the present study, pyrrhotite (Fe7S8) was investigated for the removal of Pb2+ and Cu2+ ions from aqueous solution. The Fe7S8 material was prepared through a solvothermal method and was characterized using XRD. The average particle size for the nanomaterial was determined to be 29.86 +/- 0.87 nm using XRD analysis and Scherrer's equation. Batch studies were performed to investigate the effects of pH, time, temperature, interfering ions, and the binding capacity of Pb2+ and Cu2+ ions to the Fe(7)S(8 )nanomaterial. During the pH profile studies, the optimum pH for the binding of Pb2+ and Cu2+ was determined to be pH 5 for both cations. Isotherm studies were conducted from which the thermodynamics and binding capacities for both Cu2+ and Pb2+ were determined. The binding capacity for Pb2+ and Cu2+ binding to the Fe7S8 were determined to be 0.039 and 0102 mmol/g, respectively at 25 degrees C. The thermodynamic parameters indicated a AG for the sorption of Pb2+ ranged from 5.07 kJ/mol to -2.45 kJ/mot indicating a non-spontaneous process was occurring. Whereas, the AG for Cu2+ ion binding ranged from 9.78 kJ/mot to -11.23 kJ/mol indicating a spontaneous process at higher temperatures. The enthalpy indicated an endothermic reaction was occurring for the binding of Pb2+ and Cu2+ to the Fe7S8 nanomaterial with AH values of 55.8 kJ/mol and 153.5 kJ/mol, respectively. Furthermore, the AS values for the reactions were positive indicating an increase in the entropy of the system after metal ion binding. Activation energy studies indicated the binding for both Pb2+ and Cu2+ occurred through chemisorption. Published by Elsevier B.V.
机译:在本研究中,研究了PyrrHotite(Fe7S8)以从水溶液中除去Pb2 +和Cu2 +离子。 Fe7S8材料通过溶剂质方法制备,并使用XRD表征。使用XRD分析和Scherrer等式确定纳米材料的平均粒径为29.86 +/- 0.87nm。进行批量研究以研究pH,时间,温度,干扰离子的影响,PB2 +和Cu2 +离子的结合能力与Fe(7)S(8)纳米材料。在pH谱研究期间,测定Pb2 +和Cu2 +结合的最适pH值为两个阳离子的pH5。进行了等温的研究,从中测定了Cu2 +和Pb2 +的热力学和结合容量。将PB2 +和Cu2 +与Fe7S8结合的结合能力分别在25℃下测定为0.039和0102mmol / g。热力学参数表明PB2 +吸附的AG为5.07 kJ / mol至-2.45 kJ /显示出现非自发过程的MOT。然而,Cu2 +离子结合的Ag从9.78kj / mot到-11.23 kj / mol的范围为-11.23kj / mol,表明在较高温度下的自发过程。将焓表明,用于将PB2 +和Cu 2+的结合发生吸热反应,分别具有55.8kJ / mol和153.5kJ / mol的α%的α8纳米材料。此外,作为反应的作为值是阳性表明金属离子结合后系统熵的增加。激活能量研究表明通过化学吸附发生Pb2 +和Cu2 +的结合。 elsevier b.v出版。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号