The grephene (GE)@waterborne polyurethane (WPU) microcapsule (GE@WPU) is synthesized and introduced GE@WPU microcapsules to aramid fibers (AF) surface. Compare with GE is directly added to WPU solution, the GE@WPU microcapsule suspension is improved significantly. The results show that the tensile strength (19.1 cN/dtex) of modified AF is higher than unmodified AF (17.5 cN/dtex), the elongation at break (1.47%) of modified AF is lower than the unmodified AF (1.51%); the GE@WPU microcapsules can significantly decrease the surface resistivity. Modified AF is introduced into natural rubber (NR), findings indicated that the GE@WPU microcapsule modified AF contribute to enhancing the interfacial adhesion properties of AF/NR composites, the pull-out force of modified AF/NR composites is increased with the content of GE@WPU microcapsules increase, the pull-out force (142 N/cm) of modified AF/NR composites is higher than the unmodified AF/NR composites (64 N/cm). This means that the method can be applied in the fiber-reinforced composites.
机译:合成Grephene(GE)@Waterborne聚氨酯(WPU)微胶囊(GE @ WPU)并将GE @ WPU微胶囊引入芳族纤维(AF)表面。与GE进行比较直接添加到WPU解决方案中,GE @ WPU微胶囊悬浮液显着提高。结果表明,改性AF的拉伸强度(19.1cn / dtex)高于未修饰的AF(17.5cn / dtex),断裂的伸长率(1.47%)修饰的AF低于未修饰的AF(1.51%); GE @ WPU微胶囊可以显着降低表面电阻率。改性AF被引入天然橡胶(NR)中,结果表明GE @ WPU微胶囊改性AF有助于提高AF / NR复合材料的界面粘附性,改性AF / NR复合材料的拉出力随含量增加在GE @ WPU微胶囊的增加,改性AF / NR复合材料的拉出力(142n / cm)高于未修饰的AF / NR复合材料(64N / cm)。这意味着该方法可以应用于纤维增强复合材料。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号