The Physical Simulation on Extrusion Process of Glass Fiber Composite Wire Coated by Lead

机译:铅包覆玻璃纤维复合丝挤压工艺的物理模拟

获取原文
获取原文并翻译 | 示例
           

摘要

The method of manufacturing the composite wire by extruding lead to coated glass fiber is described. The different composite wire that diameter is from 0.5 to 1.0mm has been produced by two kinds of different extruding technology (getting wire along horizontal direction and getting wire along perpendicular direction). The optimal extruding technological parameter has been given in different extruding technology by the physical simulation (H: 300t, SSOkN, 0.16mm. P: 300t, 215kN, 0.16mm). The effect on the coating speed by other extruding technological parameters in the different extruding technology has been discussed. The extruding temperature and extruding force is higher, the coating speed is faster. It has been pointed, that the affection on the extruding technology by the extruding temperature has also behaved as the extruding temperature rising up spontaneously. The reason for exiting the minimum extruding force and maximum extruding force also has been discussion in this paper. It is also important to the extruding process and coating speed that is the coating clearance.
机译:描述了通过将铅挤出到涂覆的玻璃纤维中来制造复合线材的方法。通过两种不同的挤出技术(沿水平方向取丝和沿垂直方向取丝)生产了直径为0.5至1.0mm的不同复合丝。通过物理模拟(H:300t,SSOkN,0.16mm。P:300t,215kN,0.16mm)在不同的挤出工艺中给出了最佳挤出工艺参数。讨论了不同挤出技术中其他挤出技术参数对涂布速度的影响。挤出温度和挤出力较高,涂布速度较快。已经指出,挤出温度对挤出技术的影响还表现为挤出温度自发升高。本文还讨论了退出最小挤压力和最大挤压力的原因。对于挤出过程和涂布速度,涂布间隙也很重要。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号