Various compositions of nano-sized (NiMoO_4)_x-doped Bi_2Ti_4O_(11) (x = 0.01, 0.05, 0.1) composites have been prepared by chemical solution decomposition (CSD) method using triethanolamine (TEA) as complexing agent. Ni(II) is one of reactive species on the catalyst surface and Mo(VI) ion helps to compensate the charge of the lattice. The photocatalysts based on the above compositions have been tested for photobleaching of methyl orange (MO) solution under Hg-lamp. The prepared nanopowders are characterized by XRD, EDAX, UV-vis spectra, specific surface area (BET), zeta potential, ESR and HRTEM analyses. The average particle size of nickel molybdate-doped bismuth titanate lies around 30 + - 2 nm measured from TEM. Result shows nickel molybdate-doped bismuth titanate (NiMoO_4)_x(Bi_2Ti_4O_(11))_(1-x) (NM_xBT_(1-x) x = 0.01) composite is found to be more photoactive compared all the compositions studied except degussa P25 titania.
机译:使用三乙醇胺(TEA)作为络合剂,通过化学溶液分解(CSD)方法制备了纳米(NiMoO_4)_x掺杂的Bi_2Ti_4O_(11)(x = 0.01、0.05、0.1)复合材料的各种组成。 Ni(II)是催化剂表面的反应性物质之一,Mo(VI)离子有助于补偿晶格电荷。已经测试了基于上述组合物的光催化剂在汞灯下对甲基橙(MO)溶液的光漂白。通过XRD,EDAX,紫外可见光谱,比表面积(BET),ζ电位,ESR和HRTEM分析对制备的纳米粉进行表征。从TEM测量,掺杂钼酸镍的钛酸铋铋的平均粒度为约30±2nm。结果表明,掺杂钼酸镍的钛酸铋(NiMoO_4)_x(Bi_2Ti_4O_(11))_(1-x)(NM_xBT_(1-x)x = 0.01)复合物的光活性高于除degussa P25以外的所有成分二氧化钛。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号