Effect of Thermotropic Liquid Crystalline Poly(ether ketone)arylates on the Processibility and Properties of Poly(ether ether ketone)s Fibers

机译:热致液晶聚醚醚酮芳基化物对聚醚醚酮纤维加工性能的影响

获取原文
获取原文并翻译 | 示例
           

摘要

A series of composite fibers based on poly(ether ether ketone)s (PEEK) and a thermotropic liquid crystalline poly(ether ketone)arylates (PEKAR) have been prepared by melt spinning. The structure, compatibility, and properties of these composite fibers were investigated in detail by rheological measurements, differential scanning calorimetry, thermogravimetric analysis, wide-angle X-ray diffraction, scanning electron microscopy, orientation degree test, and mechanical properties test. The results showed that the addition of PEKAR could reduce the apparent melt viscosity of the blends obviously, which is beneficial in improving the processibility of PEEK at a relatively low temperature. After adding 1 wt % PEKAR to PEEK, the tensile strength of the post-treatment fiber improved by 8.8%, whereas the crystallinity of the as-spun fiber increased from 21.76% to 31.51%, and the orientation degree also increased with the addition of PEKAR. The result of morphology research suggested that PEKAR had a good compatibility with PEEK resin.
机译:通过熔融纺丝制备了一系列基于聚醚醚酮(PEEK)和热致液晶聚醚醚基液晶(PEKAR)的复合纤维。通过流变学测量,差示扫描量热法,热重分析,广角X射线衍射,扫描电子显微镜,取向度测试和力学性能测试,详细研究了这些复合纤维的结构,相容性和性能。结果表明,加入PEKAR可以明显降低共混物的表观熔体粘度,有利于提高PEEK在较低温度下的加工性能。在PEEK中添加1 wt%的PEKAR后,后处理纤维的拉伸强度提高了8.8%,而初纺纤维的结晶度从21.76%提高至31.51%,并且取向度也随着添加PBT的增加而提高。 PEKAR。形态研究结果表明,PEKAR与PEEK树脂具有良好的相容性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号