Mechanical characteristics of swollen gellan gum hydrogels

机译:结冷胶水凝胶的力学特性

获取原文
获取原文并翻译 | 示例

摘要

The behavior of swollen gellan gum hydrogels in terms of mechanical properties, weight loss, and cell growth inhibition of leachates is presented. Low-acyl gellan gum (LAGG), high-acyl gellan gum (HAGG), and a HAGG-LAGG blend were soaked in phosphate-buffered saline (PBS) at pH 7.4 and 37°C for up to 168 days. The gels exhibited their maximum mass loss and swelling after 28 days of immersion in PBS. LAGG gels exhibited lower value for mass loss and the chain-release diffusion coefficient than gels consisting of HAGG and the HAGG-LAGG blend. The change in mechanical and rheological characteristics during soaking of the three hydrogels was attributed to mass loss, while LAGG hydrogels also showed evidence of effects because of cation exchange with the surrounding medium. The mechanical characteristics of the LAGG, HAGG, and blend hydrogels relative to each other did not change during swelling (although the magnitude changed). L929 fibroblasts growth inhibition tests showed that the leachate products of the three gels can be considered noncytotoxic, which is important for their future application in tissue engineering.
机译:提出了溶胀的结冷胶水凝胶在机械性能,重量减轻和浸出液对细胞生长的抑制方面的行为。将低酰基吉兰糖胶(LAGG),高酰基吉兰糖胶(HAGG)和HAGG-LAGG混合物在pH 7.4和37°C的磷酸盐缓冲液(PBS)中浸泡最多168天。浸入PBS 28天后,凝胶表现出最大的质量损失和溶胀。与由HAGG和HAGG-LAGG共混物组成的凝胶相比,LAGG凝胶的质量损失和链释放扩散系数更低。三种水凝胶在浸泡过程中机械和流变特性的变化归因于质量损失,而LAGG水凝胶由于与周围介质的阳离子交换也显示出影响的证据。在膨胀过程中,LAGG,HAGG和共混水凝胶相对于彼此的机械特性没有改变(尽管大小发生了变化)。 L929成纤维细胞生长抑制试验表明,三种凝胶的渗滤液产物可被视为无细胞毒性,这对于它们在组织工程中的未来应用非常重要。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号