A copolymer of phenylisocyanate (PhNCO) and epsilon-caprolactone (CL) was synthesized by the rare earth chloride systems lanthanide chloride isopropanol complex (LnCl(3)center dot 3iPrOH) and propylene epoxide (PO). Polymerization conditions were investigated, such as lanthanides, reaction temperature, monomer feed ratio, La/PO molar ratio, and aging time of catalyst. The optimum conditions were: LaCl3 preferable, [PhNCO]/[CL] in feed = I (molar ratio), 30 degrees C, [monomer]/[La] 200, [PO]/[La]=20, aging 15 min, polymerization in bulk for 6 h. Under such conditions the copolymer obtained had 39 mol % PhNCO with a 78.2% yield, M-n=20.3 x 10(3), and M-w/M-n = 1.60. The copolymers were characterized by GPC, TGA, H-1-NMR, and C-13-NMR, and the results showed that the copolymer obtained had a blocky structure with long sequences of each monomer unit. (c) 2006 Wiley Periodicals, Inc. I Appl Polym Sci 103: 2135-2140, 2007
机译:通过稀土氯化物镧系氯化物异丙醇配合物(LnCl(3)中心点3iPrOH)和环氧丙烷(PO)合成了异氰酸苯酯(PhNCO)和ε-己内酯(CL)的共聚物。研究了聚合条件,例如镧系元素,反应温度,单体进料比,La / PO摩尔比和催化剂的老化时间。最佳条件为:优选LaCl3,进料中的[PhNCO] / [CL] = I(摩尔比),30摄氏度,[单体] / [La] 200,[PO] / [La] = 20,陈​​化15分钟,本体聚合6小时。在这样的条件下,获得的共聚物具有39mol%的PhNCO,产率为78.2%,M-n = 20.3×10(3),并且M-w / M-n = 1.60。通过GPC,TGA,H-1-NMR和C-13-NMR对共聚物进行了表征,结果表明所获得的共聚物具有嵌段结构,每个单体单元的序列较长。 (c)2006 Wiley Periodicals,Inc. I Appl Polym Sci 103:2135-2140,2007年

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号