The hydrogenation of natural rubber (NR) and various epoxidized natural rubbers (ENR) was investigated by using diimide generated in situ from the thermal decomposition of p-toluenesulfonylhydrazide (TSH) in o-xylene solution at 135degreesC. H-1-NMR analysis indicated that approximately 85-95% of hydrogenation was performed with a twofold excess of TSH. FT-IR and Raman spectroscopy were employed to confirm the microstructure characteristics of the hydrogenated rubbers. The cis-trans isomerization was also observed by H-1- and C-13-NMR. The signal in H-1-NMR of the epoxide group of the ENR disappears after hydrogenation while the signal of the opened epoxide ring product was detected. This may be due to the epoxide ring opening reaction caused by the p-toluenesulfinic acid by-product. The high temperature of the reaction condition leads to chain degradation in both NR and ENR. Thermal behaviors of the hydrogenated rubbers characterized by differential scanning calorimetry showed that the glass transition temperatures of the hydrogenated rubbers were increased about 10-20degreesC compared with the starting rubbers. (C) 2004 Wiley Periodicals, Inc.
机译:通过使用对甲苯磺酰肼(TSH)在邻二甲苯溶液中在135℃下热分解原位生成的二酰亚胺,研究了天然橡胶(NR)和各种环氧化天然橡胶(ENR)的氢化。 H-1-NMR分析表明,在两倍过量的TSH下进行了大约85-95%的氢化。 FT-IR和拉曼光谱被用来确认氢化橡胶的微观结构特征。还通过H-1-和C-13-NMR观察到顺-反异构化。氢化后,ENR的环氧基的H-1-NMR信号消失,同时检测到开环的环氧化物的信号。这可能是由于对甲苯磺酸副产物引起的环氧化物开环反应。反应条件的高温导致NR和ENR均发生链降解。通过差示扫描量热法表征的氢化橡胶的热行为表明,与起始橡胶相比,氢化橡胶的玻璃化转变温度提高了约10-20℃。 (C)2004年Wiley Periodicals,Inc.

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号