Highly purified cellulose preparations were obtained by pretreatment of dewaxed barley straw, oil palm frond fiber, poplar wood, maize stems, wheat straw, rice straw, and rye straw with 2.0% H2O2 at 45° C and pH 11.6 for 16 h, and sequential purification with 80% acetic acid-70% nitric acid (10/1, v/v) at 120° C for 15 min. The purified cellulose obtained was relatively free of bound hemicelluloses (2.3-3.2%) and lignin (0.4-0.6%) and had a yield of 35.5% from barley straw, 39.6% from oil palm frond fiber, 40.8% from poplar wood, 36.0% from maize stems, 34.1% from wheat straw, 23.40% from rice straw, and 35.8% from rye straw. The weight-average molecular weights of the purified cellulose ranged from 39,030 to 48,380 g/mol. The thermal stability of the purified cellulose was higher than that of the corresponding crude cellulose. In comparison, the isolated crude and purified cellulose samples were also studied by Fourier transform IR and cross-polarization/magic-angle spinning C-13-NMR spectroscopy. © 2005 Wiley Periodicals, Inc. J Appl Polym Sci 97: 322-335, 2005.
机译:高纯度的纤维素制剂是通过将脱蜡的大麦秸秆,油棕叶纤维,杨木,玉米茎,小麦秸秆,稻草和黑麦秸秆在45℃和2.0%H2O2的预处理下制得的; C和pH 11.6持续16小时,并在120℃用80%乙酸-70%硝酸(10/1,v / v)依次纯化; C持续15分钟。获得的纯化纤维素相对不含键合的半纤维素(2.3-3.2%)和木质素(0.4-0.6%),大麦秸秆的收率为35.5%,油棕叶纤维的收率为39.6%,白杨木的收率为40.8%,36.0玉米茎,小麦秸秆占34.1%,稻草占23.40%,黑麦草占35.8%。纯化的纤维素的重均分子量为39,030至48,380 g / mol。纯化的纤维素的热稳定性高于相应的粗纤维素的热稳定性。相比之下,还通过傅立叶变换红外光谱和交叉极化/魔角旋转C-13-NMR光谱研究了分离的粗制和纯化纤维素样品。 &复制; 2005 Wiley Periodicals,Inc.J Appl Polym Sci 97:322-335,2005。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号