Synthesis of NaLa(MoO4)2:Eu~(3+)/Yb~(3+) Phosphors via Microwave-Modified Sol-Gel Route and Their Upconversion Photoluminescence Properties

机译:微波修饰的溶胶-凝胶法合成NaLa(MoO4)2:Eu〜(3 +)/ Yb〜(3+)荧光粉及其上转换光致发光性能

获取原文
获取原文并翻译 | 示例
       

摘要

NaLa_(1-x)(MoO4)2:Eu~(3+)/Yb~(3+) phosphors with doping concentrations of En~(3+) and Yb~(3+) (x = Eu~(3+) + Yb~(3+), Eu~(3+) = 0.05, 0.1. 0.2 and Yb~(3+) = 0.2, 0.45) were successfully synthesized via the microwave-modified sol-gel route and the upconversion and spectroscopic properties were investigated. Well-crystallized particles showed a fine and homogeneous morphology with particle sizes of 5-10 urn. Under excitation at 980 nm, NaLa_(0.5)(MoO4)2:Er_(0.05)Yb_(0.45) particles exhibited a strong 525 nm emission band and a weak 550 nm emission band in the blue region and a very weak 655 nm emission band in the red region. The Raman spectra of NaLa_(0.8)(MoO4)2:Eu_(0.2), NaLa_(0.7)(MoO4):Eu_(0.1)Yb_(0.2) and NaLa_(0.5)(MoO4)2:Eu_(0.45)Yb_(0.45) particles indicated the domination of strong peaks at higher frequencies (762, 890, 1358 and 1430 cm~(-1)) and weak peaks at lower frequencies (323, 388 and 450 cm~(-1)).
机译:NaLa_(1-x)(MoO4)2:Eu〜(3 +)/ Yb〜(3+)荧光粉,掺杂浓度为En〜(3+)和Yb〜(3+)(x = Eu〜(3+ )+微波修饰的溶胶-凝胶法及上转换和光谱法成功合成了Yb〜(3+),Eu〜(3+)= 0.05,0.1。0.2和Yb〜(3+)= 0.2,0.45)性能进行了调查。结晶良好的颗粒显示出细小且均匀的形态,粒径为5-10微米。在980 nm激发下,NaLa_(0.5)(MoO4)2:Er_(0.05)Yb_(0.45)粒子在蓝色区域表现出很强的525 nm发射带和550 nm弱的发射带,以及655 nm的非常弱的发射带在红色区域。 NaLa_(0.8)(MoO4)2:Eu_(0.2),NaLa_(0.7)(MoO4):Eu_(0.1)Yb_(0.2)和NaLa_(0.5)(MoO4)2:Eu_(0.45)Yb_( 0.45)颗粒表示在较高频率(762、890、1358和1430 cm〜(-1))上的强峰和在较低频率(323、388和450 cm〜(-1))上的弱峰占主导地位。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号