A novel ceramic membrane coated with MnO2-Co3O4 nanoparticles catalytic ozonation for benzophenone-3 degradation in aqueous solution: Fabrication, characterization and performance

机译:MnO2-Co3O4纳米颗粒包覆的新型陶瓷膜催化臭氧化处理水溶液中二苯甲酮-3的降解,表征和性能

获取原文
获取原文并翻译 | 示例
           

摘要

A novel ceramic membrane coated with MnO2-Co3O4 nanoparticles was fabricated by catalytic ozonation for degradation of benzophenone-3, a typical ultraviolet absorber, from water. Synthesized MnO2-Co3O4 nanoparticles showed excellent catalytic activity. Structure and surface property characterization confirmed the presence of MnO2-Co3O4 nanoparticles with 7.05 +/- 0.99 nm diameters and a surface area as 90.0609 m(3)/g. These nanoparticles were suitable for the surface modification of ceramic membranes used in this study. Energy dispersive X-ray spectroscopy and atomic force microscopy analyses suggest that MnO2-Co3O4 nanoparticles filled membrane pores and reduced the surface roughness. The ceramic membrane coated with MnO2-Co3O4 nanoparticles showed remarkable activity in catalytic ozonation. The performance of the membrane and its surface nanoparticle layers were stable and the concentration of leached metal ions was low. After catalytic ozonation with the coated ceramic membrane, a reduction in toxicity was observed. The ceramic membrane coated with MnO2-Co3O4 nanoparticles catalytic ozonation is optional for BP-3 degradation from aqueous. (C) 2015 Elsevier B.V. All rights reserved.
机译:通过催化臭氧化作用,从水中降解典型的紫外线吸收剂二苯甲酮-3,制得了一种新型的包覆有MnO2-Co3O4纳米颗粒的陶瓷膜。合成的MnO2-Co3O4纳米颗粒表现出优异的催化活性。结构和表面性质表征确认存在MnO2-Co3O4纳米粒子,其直径为7.05 +/- 0.99 nm,表面积为90.0609 m(3)/ g。这些纳米粒子适用于本研究中使用的陶瓷膜的表面改性。能量色散X射线光谱和原子力显微镜分析表明,MnO2-Co3O4纳米粒子填充了膜孔并降低了表面粗糙度。涂覆有MnO2-Co3O4纳米颗粒的陶瓷膜在催化臭氧氧化中表现出显着的活性。膜及其表面纳米颗粒层的性能稳定,并且浸出的金属离子的浓度低。用涂覆的陶瓷膜催化臭氧氧化后,观察到毒性降低。涂覆MnO2-Co3O4纳米颗粒催化臭氧化的陶瓷膜对于BP-3从水溶液中降解是可选的。 (C)2015 Elsevier B.V.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号