In this paper, fatigue crack growth behaviour of ferritic ductile cast iron containing 3.26%C and 4.18%Si was studied. Materials were produced and reverse bending fatigue test specimens were cut from the casting with the thickness of 24 mm. Process annealing heat treatment was applied to the specimens. Semi-elliptical surface cracks were formed and reverse bending fatigue tests were carried out. Fatigue crack growth rates were determined. Stress intensity factors (Delta K) were obtained by Newman-Raju's equations. Fatigue crack growth material constants (n and c) were determined in Paris-Erdogan's equation. Fractured surfaces of the specimens were examined by using SEM. (C) 2007 Elsevier B.V. All rights reserved.
机译:本文研究了含3.26%C和4.18%Si的铁素体球墨铸铁的疲劳裂纹扩展行为。生产材料,并从铸件上切出24毫米厚的反向弯曲疲劳测试样品。对样品进行了工艺退火热处理。形成了半椭圆形的表面裂纹,并进行了反向弯曲疲劳试验。确定疲劳裂纹的增长率。应力强度因子(Delta K)通过Newman-Raju方程获得。疲劳裂纹扩展材料常数(n和c)由Paris-Erdogan方程确定。通过使用SEM检查样品的断裂表面。 (C)2007 Elsevier B.V.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号