PURPOSE: To compare the first-throw tension holding property of two braided absorbable sutures commonly used in oculoplastic surgery. METHODS: The study was an in vitro experimental model. 6/0 Polyglycolic acid (Dexon S) and 6/0 Polyglactin 910 (Coated Vicryl) were compared using an experimental model to determine first-throw knot security. A polypropylene suture (Surgipro 2) was included as a benchmark to judge the apparatus by, ensuring that our experiment could be designed independently of the test suture materials. Increasing metric loads were applied to the first double throw of a surgical knot. Each suture was tested to the point of knot slipping and the critical tension recorded. All the sutures were kept wet during use. Three variations of the experiment were undertaken: experiment 1 -- two metal loops brought together by the test suture; experiment 2 -- two strips of tissue brought together by the test suture; and experiment 3 -- a knot tied over a metal bar coated in tissue. The tissue used was processed cross-linked porcine dermal collagen (Permacol). Each experiment was repeated three times for each suture type and the mean value taken. RESULTS: Experiment 1: Dexon S 12.2 g (11, 12, 13.5), Coated Vicryl 2.5 g (2.5, 2.5, 2.5) and Surgipro 2 2.3 g (2, 2, 3); experiment 2: Dexon S 33.33 g (30, 35, 35), Coated Vicryl 25 g (25, 25, 25) and Surgipro 2 5 g (5, 5, 5); experiment 3: Dexon S 100 g (100, 100, 100), Coated Vicryl 56.667 g (60, 55, 55) and Surgipro 2 5 g (5, 5, 5). CONCLUSIONS: Dexon S-braided absorbable suture has significantly better first-throw knot security when compared with Coated Vicryl. This is an important property when suturing tissues under tension as it minimizes slippage before the locking throw is tied.
机译:目的:比较在眼部整形外科中常用的两种编织的可吸收缝合线的初抛张力保持特性。方法:该研究是体外实验模型。使用实验模型比较了6/0聚乙醇酸(Dexon S)和6/0 polyglactin 910(包衣的Vicryl),以确定首掷结安全性。聚丙烯缝线(Surgipro 2)作为基准来判断设备,以确保我们的实验可以独立于测试缝线材料进行设计。公制负载的第一次双掷增加了公制负载。测试每个缝合线至打结点并记录临界张力。在使用过程中,所有缝线均保持湿润。进行了三个实验变体:实验1 –测试缝线将两个金属环连接在一起;实验2-通过测试缝线将两条组织合在一起;实验3:打结,用金属棒包裹组织。使用的组织是经过加工的交联猪真皮胶原蛋白(Permacol)。对于每种缝合线类型,将每个实验重复三遍,并取平均值。结果:实验1:Dexon S 12.2 g(11、12、13.5),包衣的Vicryl 2.5 g(2.5、2.5、2.5)和Surgipro 2 2.3 g(2、2、3);实验2:Dexon S 33.33 g(30,35,35),包衣的Vicryl 25 g(25,25,25)和Surgipro 2 5 g(5,5,5);实验3:Dexon S 100克(100、100、100),包衣的Vicryl 56.667克(60、55、55)和Surgipro 2 5克(5、5、5)。结论:与涂层Vicryl相比,Dexon S编织可吸收缝合线具有更好的首发结安全性。当在张力下缝合组织时,这是一个重要的属性,因为它可以最大程度地减少在绑紧锁栓之前的打滑。