Biomechanical and histological evaluation of four different titanium implant surface modifications: An experimental study in the rabbit tibia

机译:四种不同钛种植体表面修饰的生物力学和组织学评估:兔胫骨的实验研究

获取原文
获取原文并翻译 | 示例
获取外文期刊封面目录资料

摘要

Objectives: This study presents a biomechanical comparison of bone response to commercially pure titanium screws with four different types of surface topographies placed in the tibial metaphysis of 30 rabbits. Materials and methods: One hundred twenty implants were tested double-blinded: (a) blasted, acid-etched, and discrete crystal deposition (DCD), (b) blasted, (c) acid-etched, and (d) blasted and acid-etch. Resonance frequency analysis (RFA/ISQ), reverse torque values (RTV), and bone-to-implant contact (BIC) were measured at the time of implant insertion (day 0), 15, 28, and 56 days of healing. Results: All groups tested demonstrated increased RFA/ISQ and RTV results over the time course. At 15 days, the blasted, acid-etched, and DCD group demonstrated a non-significant trend toward higher values when compared to the blasted and etched group (33.0 ± 16 vs. 26.3 ± 12 Ncm, p =.16). At 56 days, the groups utilizing blasting to create additional surface roughness (Sa > 1 micron) showed a statistical significant difference in RTQ versus the non-blasted group (38.5 ± 14 vs. 29.5 ± 9 Ncm, p =.03). Conclusions: Within the limitations of this study, only the increase in surface roughness (Ra > 1) at 56 days demonstrated statistically significant effects on RTQ. Other additional surface features, such as sub-micron scale DCD, demonstrated improved healing trends but without significance for clinical applications.
机译:目的:这项研究提出了对商业纯钛螺钉的骨反应的生物力学比较,钛螺钉具有四种不同类型的表面形貌,放置在30只兔子的胫骨干physi端。材料和方法:对120个植入物进行了双盲测试:(a)喷砂,酸蚀和离散晶体沉积(DCD),(b)喷砂,(c)酸蚀,以及(d)喷砂和酸蚀-蚀刻。在植入植入物(愈合的第0天),愈合的第15天,第28天和第56天时测量共振频率分析(RFA / ISQ),反向扭矩值(RTV)和骨与植入物的接触(BIC)。结果:所有测试组均显示随时间变化的RFA / ISQ和RTV结果增加。与喷砂和蚀刻组相比,喷砂,酸蚀和DCD组在15天时显示出较高值的非显着趋势(33.0±16对26.3±12 Ncm,p = .16)。在第56天,利用喷砂处理产生额外表面粗糙度(Sa> 1微米)的组与未经喷砂处理的组在RTQ上显示出统计学上的显着差异(38.5±14 vs. 29.5±9 Ncm,p = .03)。结论:在本研究的范围内,仅在56天时表面粗糙度的增加(Ra> 1)表现出对RTQ的统计学显着影响。其他附加的表面特征,例如亚微米级DCD,显示出改善的愈合趋势,但对临床应用没有意义。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号