Starting from ZrN and amorphous boron, dense ZrB2 ceramics with 37 vol% hexagonal BN were consolidated by spark plasma sintering. Benefiting from the moderate exothermic reaction between ZrN and B and the resultant fine powder generated, ZrB2-BN ceramics with relative density of 94% could be reached at 1100 degrees C, further improved to 97% by 1550 degrees C. The effects of sintering temperature and holding time on the densification behavior, microstructural evolution and mechanical properties of ZrB2-BN ceramics were investigated. ZrB2-37 vol%BN ceramics densified at 1700 degrees C exhibited attractive mechanical performance: a three-point bending strength of 353 MPa, a Vicker's hardness of 6.7 GPa and a Young's modulus of 197.5 GPa. Note that its strength dropped sharply to 191 MPa measured at 1300 degrees C. The combination of low sintering temperature (1100-1550 degrees C), low Young's modulus (180-200 GPa) and relatively high strength (200-350 MPa) make reactively sintered ZrB2-BN composites as promising matrix for continuous fiber reinforced composites. (C) 2016 Elsevier Ltd. All rights reserved.
机译:从ZrN和非晶态硼开始,通过火花等离子烧结固结了具有37%(体积)六方BN的致密ZrB2陶瓷。得益于ZrN和B之间的适度放热反应和生成的细粉,可以在1100摄氏度下达到94%相对密度的ZrB2-BN陶瓷,到1550摄氏度可以进一步提高到97%。烧结温度的影响并研究了保温时间对ZrB2-BN陶瓷致密化行为,微观组织演变和力学性能的影响。在1700摄氏度下致密的ZrB2-37 vol%BN陶瓷具有吸引人的机械性能:三点弯曲强度为353 MPa,维氏硬度为6.7 GPa,杨氏模量为197.5 GPa。请注意,它的强度在1300摄氏度下测量时急剧下降至191 MPa。低烧结温度(1100-1550摄氏度),低杨氏模量(180-200 GPa)和相对较高的强度(200-350 MPa)相结合烧结ZrB2-BN复合材料作为连续纤维增强复合材料的有希望的基质。 (C)2016 Elsevier Ltd.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号