The undoped and Ce-doped LiF/LiLuF_4 eutectic fibers with various ratios of LuF_3 to LiF were grown by the micro-pulling-down method for their application as neutron scintillators with light guiding structure. The differential thermal analysis (DTA) of undoped eutectic materials indicated that the eutectic point of LiF/LiLuF_4 was positioned around LiF 80 mol%-LuF_3 20 mol% composition. Some of the as-produced eutectic solids had rod-like regular array structures. This was observed using SEM images of cross-sectional and parallel cuts of the grown solids. In the range of x ≥ 0.28, the dendrites appeared between the eutectic areas. Ce doped LiF/LiLuF_4 eutectic fibers demonstrated two emission peaks around 310 and 326 nm in the photoluminescence spectrum, and the decay time of the emission at 326 nm was 32.3 ns.
机译:通过微下拉法生长了具有不同LuF_3与LiF比值的未掺杂和铈掺杂的LiF / LiLuF_4共晶纤维,以用作具有光导结构的中子闪烁体。未掺杂共晶材料的差热分析(​​DTA)表明,LiF / LiLuF_4的共晶点位于LiF 80 mol%-LuF_3 20 mol%组成附近。一些刚产生的共晶固体具有棒状规则阵列结构。使用生长的固体的横截面和平行切口的SEM图像观察到了这一点。在x≥0.28的范围内,在共晶区域之间出现树枝状晶体。 Ce掺杂的LiF / LiLuF_4共晶纤维在光致发光光谱中显示出在310和326 nm附近的两个发射峰,并且在326 nm处的发射衰减时间为32.3 ns。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号