The present paper deals with the processing method of SiC-(Nb,Ti)_(ss)-(Ti,Nb)C_(ss) composites. The electrically conductive phases were formed by in situ reaction: NbC_(s) + Ti_(s)- > (Nb,Ti)_(ss) + (Ti,Nb)C_(ss) that takes place during the reaction sintering by hot pressing. Prepared composites exhibit good compromise between electrical and mechanical properties and the present approach allows preparing a wide variety of compositions. For example composites containing 80 wt. percent SiC and 20 wt. percent {(Nb.Ti)_(ss)-(Ti,Nb)C_(ss)} have an electrical resistivity 2.6 X 10~(-4) OMEGA m, hardness 21.6 GPa and fracture toughness 6.3 MPam~(1/2).
机译:本文研究了SiC-(Nb,Ti)_(ss)-(Ti,Nb)C_(ss)复合材料的加工方法。导电相通过原位反应形成:NbC_(s)+ Ti_(s)->(Nb,Ti)_(ss)+(Ti,Nb)C_(ss),该反应在热烧结过程中发生紧迫。制备的复合材料在电性能和机械性能之间表现出良好的折衷,并且本发明的方法允许制备各种各样的组合物。例如,包含80重量%的复合材料。 SiC含量和20 wt。百分比{(Nb.Ti)_(ss)-(Ti,Nb)C_(ss)}的电阻率为2.6 X 10〜(-4)OMEGA m,硬度为21.6 GPa,断裂韧性为6.3 MPam〜(1/2) )。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号