To determine the effect of ZnO in ZnO-containing fayalite (ZFS) slags on the degradation of magnesia-chromite refractories, the corrosion behaviour of a direct-bonded magnesia-chromite refractory was studied by rotating refractory finger tests at 1200 degrees C under reducing atmosphere. In addition, MgO crucible tests at these conditions were performed to investigate in particular the effect of ZnO on the slag/MgO interaction. The dissolution of MgO from periclase into the ZFS slags is not enhanced by increasing the ZnO content in the slags. (Fe,Mg,Zn)(2)SiO4 olivine and (Fe,Mg,Zn)O solid solution are the only two products in the slag/MgO interfacial reactions,"even when the ZnO content in the ZFS slag reaches 16.7 wt%. The diffusion of ZnO into the chromite grains to form the (Fe,Mg,Zn)(Fe,Al,Cr)(2)O-4 spinel was favoured with increasing the ZnO content in ZFS slags. (C) 2016 Elsevier Ltd. All rights reserved.
机译:为了确定含ZnO的铁橄榄石(ZFS)炉渣中ZnO对镁铬铁质耐火材料降解的影响,通过在还原气氛下于1200摄氏度下旋转耐火手指试验研究了直接粘结的镁铬铁质耐火材料的腐蚀行为。 。此外,在这些条件下进行了MgO坩埚测试,以特别研究ZnO对炉渣/ MgO相互作用的影响。通过增加矿渣中ZnO的含量,并不能增强MgO从过氧化物酶到ZFS矿渣中的溶解。 (Fe,Mg,Zn)(2)SiO4橄榄石和(Fe,Mg,Zn)O固溶体是炉渣/ MgO界面反应中仅有的两种产物,即使ZFS炉渣中的ZnO含量达到16.7 wt% ZnO扩散到铬铁矿晶粒中形成(Fe,Mg,Zn)(Fe,Al,Cr)(2)O-4尖晶石有助于增加ZFS渣中ZnO的含量。(C)2016 Elsevier Ltd 。 版权所有。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号