In this study, three different industrial frits BaO-Al_2O_3-SiO_2 (BAS), CaO-MgO-Al_2O_3-SiO_2 (CMAS), CaO-ZrO_2-Al_2O_3-SiO_2 (CZAS) have been deposited on porcelainized stoneware tiles by plasma spraying. In the as-sprayed conditions, the microstructure of the coatings is defective because of pores, microcracks and low intersplat cohesion. Hot stage microscope and differential thermal analysis measurements made on the glass powders allowed to characterize the frits thermal behaviour. Post process thermal treatments have been arranged, following these indications as well as preliminary tests, in order to achieve the lowest porosity and the highest resistance to abrasion. At the chosen temperatures, a microstructural improvement has been induced, but in the BAS specimens, an optimal sintering has not been accomplished because of the unavoidable full overlapping of the sintering and crystallization processes.
机译:在这项研究中,已通过等离子喷涂将三种不同的工业玻璃料BaO-Al_2O_3-SiO_2(BAS),CaO-MgO-Al_2O_3-SiO_2(CMAS),CaO-ZrO_2-Al_2O_3-SiO_2(CZAS)沉积在瓷质瓷砖上。在喷涂状态下,涂层的微观结构由于孔,微裂纹和低的板间结合力而有缺陷。在玻璃粉上进行的热台显微镜和差热分析测量可以表征玻璃料的热行为。根据这些指示以及初步测试,已经安排了后处理热处理,以实现最低的孔隙率和最高的耐磨性。在选定的温度下,已经引起了微观结构的改善,但是在BAS样品中,由于不可避免地发生烧结和结晶过程的完全重叠,因此尚未实现最佳烧结。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号