首页> 外文期刊>Journal of Renewable Materials >Photodegradation of Polyurethane Foam Obtained from Renewable Resource-Pulp Production Byproducts
【24h】

Photodegradation of Polyurethane Foam Obtained from Renewable Resource-Pulp Production Byproducts

机译:从可再生资源纸浆生产副产物中获得的聚氨酯泡沫的光降解

获取原文
获取原文并翻译 | 示例
           

摘要

Rigid polyurethane foams were obtained from pulp production byproducts. Three different polyols were used—tall oil polyol, lignopolyol and commercially available polyol for comparison. The obtained rigid polyurethane foams underwent photodegradation at 60°C temperature and at 0.89 W/m2 intensity of UV light radiation up to 1000 h. Changes in chemical structure were observed by Fourier Transform Infrared Spectroscopy and Scanning Electron Microscopy was used to study changes in cell morphology. Spectrophotometery was used to determine yellowing of the foams. Results showed that the thickness of degraded layer for rigid polyurethane foams obtained from pulp production byproducts was ~25% less than for foams from commercially available polyol. Overall results suggest that rigid polyurethane foams from lignopolyol show better performance against photodegradation.
机译:硬质聚氨酯泡沫是从纸浆生产副产品获得的。为了比较,使用了三种不同的多元醇-妥尔油多元醇,木质素多元醇和市售多元醇。所获得的硬质聚氨酯泡沫在60°C的温度下以1000小时的0.89 W / m2的紫外线辐射强度进行光降解。通过傅立叶变换红外光谱观察化学结构的变化,并使用扫描电子显微镜研究细胞形态的变化。用分光光度计测定泡沫的泛黄。结果表明,由纸浆生产副产品获得的硬质聚氨酯泡沫的降解层厚度比市售多元醇的泡沫低约25%。总体结果表明,木质素多元醇制得的硬质聚氨酯泡沫具有更好的抗光降解性能。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号