SHORT BANANA FIBER REINFORCED POLYESTER COMPOSITES - MECHANICAL, FAILURE AND AGING CHARACTERISTICS

机译:香蕉皮短纤维增强聚酯复合材料-机械,破坏和老化特性

获取原文
获取原文并翻译 | 示例
           

摘要

This paper describes the tensile, impact, flexural properties and aging behavior of short banana fiber reinforced polyester composites with Special reference to the effect of fiber length and fiber content. Maximum tensile strength was observed at 30 mm fiber length while impact strength gave the maximum value for 30 mm fiber length. Incorporation of 40% untreated fibers gave a 20% increase in the tensile strength and a 341% increase in impact strength. On treatment with silane coupling agent, composites showed a 28% increase in tensile strength and a 13% increase in flexural strength. Aging studies showed a decrease in tensile strength of the composites, The experimental tensile strength values were compared with theoretical predictions according to Piggot equation, Scanning electron microscopy studies were carried out to understand the morphology of the fiber surface, fiber pullout and interface bonding. Water absorption studies showed an increase in water uptake with increase in fiber content. Finally, the properties of banana fiber reinforced polyester composites have been compared with other natural fiber reinforced composites. [References: 33]
机译:本文介绍了短香蕉纤维增强聚酯复合材料的拉伸,冲击,弯曲性能和老化行为,并特别参考了纤维长度和纤维含量的影响。在30 mm纤维长度处观察到最大拉伸强度,而冲击强度在30 mm纤维长度处达到最大值。掺入40%未经处理的纤维可使抗张强度提高20%,冲击强度提高341%。经硅烷偶联剂处理后,复合材料的拉伸强度提高了28%,弯曲强度提高了13%。老化研究表明复合材料的拉伸强度降低,根据Piggot方程将实验拉伸强度值与理论预测值进行了比较,进行了扫描电子显微镜研究以了解纤维表面的形态,纤维的拉拔和界面结合。吸水率研究表明,吸水率随纤维含量的增加而增加。最后,将香蕉纤维增强聚酯复合材料的性能与其他天然纤维增强复合材料进行了比较。 [参考:33]

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号