The microstructure, magnetic and electrical transport properties of La0.67Sr0.33MnO3/Nd0.67Sr0.33MnO3 composites are studied as a function of sintering temperature. At 900degreesC, the intergrain exchange couplings between the adjacent particles give rise to an increase in resistance. Raising the sintering temperature induces the formation of an interfacial phase near the La0.67Sr0.33MnO3 and Nd0.67Sr0.33MnO3 grain boundaries as indicated in the XRD pattern and SEM image. At 1100degreesC, the formation of interfacial phases near the grain boundaries enhances the conductivity in the composite. Broad magnetoresistance across room temperature is observed in a composite sintered at 1300degreesC. This observation may be ascribed to the coexistence of multiphase in the composite which leads to a decrease in resistance. The results suggest that sintering temperature has a prominent effect on the properties of the grain boundary, which plays an important role in determining the electrical transport behaviour of the composites.
机译:研究了La0.67Sr0.33MnO3 / Nd0.67Sr0.33MnO3复合材料的微观结构,电磁输运性能与烧结温度的关系。在900℃下,相邻颗粒之间的晶粒间交换偶合引起电阻的增加。如XRD图和SEM图像所示,提高烧结温度导致在La0.67Sr0.33MnO3和Nd0.67Sr0.33MnO3晶界附近形成界面相。在1100℃下,晶界附近界面相的形成增强了复合材料的电导率。在1300℃下烧结的复合材料中观察到了跨越室温的宽磁阻。该观察结果可归因于复合物中多相的共存,这导致电阻降低。结果表明,烧结温度对晶界性能有显着影响,这在决定复合材料的电输运行为中起着重要作用。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号