首页> 外文期刊>Journal of oral rehabilitation >Marginal and internal fit of all-ceramic CAD/CAM crown-copings on chamfer preparations.
【24h】

Marginal and internal fit of all-ceramic CAD/CAM crown-copings on chamfer preparations.

机译:全陶瓷CAD / CAM顶盖在切角准备上的边缘和内部配合。

获取原文
获取原文并翻译 | 示例
           

摘要

Evaluation of the marginal and internal fit of all-ceramic molar crown-copings hypothesizing that Computer Aided Design/Computer Aided Manufacturing (CAD/CAM) fabrication shows the same accuracy of fit as conventional techniques. A set of six individual crown preparations was duplicated 12 times yielding 72 plaster dies. Slip-cast (In-Ceram Zirconia), heat-pressing (Empress II) and CAD/CAM crown-copings (Cerec inLab, DCS, Decim and Procera) were seated on 12 dies each. Marginal and internal gap width was measured in the SEM at 120x magnification. Marginal gap of slip-cast (25 +/- 18 microm) was significantly (P < 0.05) smaller than that of Empress II (44 +/- 23 microm) copings. Procera (17 +/- 16 microm) and Decim (23 +/- 17 microm) did not differ (P > 0.05) from slip-cast (25 +/- 18 microm) but were smaller (P < 0.001/P < 0.01) than Empress II (44 +/- 23 microm) and Cerec inLab (43 +/- 23 microm) (P < 0.001/P < 0.05). DCS (33 +/- 20 microm) did not differ (P > 0.05) from any of the others. The internal mid-orobuccal gap width of Procera (136 +/- 68 microm) was larger (P < 0.001) than that of Decim (81 +/- 30 microm) and slip-cast (94 +/- 84 microm) (P < 0.05) while Empress II (105 +/- 53 microm), DCS (110 +/- 79 microm) and Cerec inLab (114 +/- 58 microm) did not differ significantly (P > 0.05) from Decim, Procera and slip-cast. Internal mesiodistal gap width was similar. The fit of conventional and CAD/CAM all-ceramic molar crown-copings covered the same range of gap width confirming the assumed hypothesis.
机译:假设计算机辅助设计/计算机辅助制造(CAD / CAM)加工显示出与传统技术相同的贴合精度,因此对所有陶瓷磨牙冠冠的边缘和内部贴合进行评估。将一组六个单独的牙冠制剂重复12次,得到72个石膏模。滑模铸造(In-Ceram氧化锆),热压成型(Empress II)和CAD / CAM冠状套色(Cerec inLab,DCS,Decim和Procera)分别安装在12个模具上。在SEM中以120倍放大率测量边缘和内部间隙宽度。滑模铸件的边际间隙(25 +/- 18微米)显着(P <0.05)比Empress II的边际间隙(44 +/- 23微米)要小。 Procera(17 +/- 16微米)和Decim(23 +/- 17微米)与滑模铸造(25 +/- 18微米)没有差异(P> 0.05),但较小(P <0.001 / P <0.01 )(Empress II(44 +/- 23微米)和Cerec inLab(43 +/- 23微米)(P <0.001 / P <0.05)。 DCS(33 +/- 20微米)与其他任何一个都没有差异(P> 0.05)。 Procera的口腔内中间隙宽度(136 +/- 68微米)大于Decim(81 +/- 30微米)和滑模(94 +/- 84微米)(P <0.001)(P <0.05),而Empress II(105 +/- 53微米),DCS(110 +/- 79微米)和Cerec inLab(114 +/- 58微米)与Decim,Procera和支路没有显着差异(P> 0.05) -投。内部近中隔间隙宽度相似。常规和CAD / CAM全陶瓷磨牙牙冠的拟合覆盖了相同的间隙宽度范围,从而证实了假设。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号