Composition change during the melting process of some glasses in the PbBr2-PbCl2-PbF2-PbO-P2O5 system melted at 450-470 degreesC for 15 min was studied. Results show that there was a remarkable difference between the batch composition and the analyzed composition. Large amount of P, Br, Pb, and Cl were lost mainly in the form of PbBr2, PbCl2 and P2O5. The content of O is influenced by two factors. The incomplete decomposition of NH4H2PO4 or the reaction between P2O5 and H2O in the atmosphere increases the content of O, while the volatilization of P2O5 decreases the content of O. (C) 2001 Elsevier Science B.V. All rights reserved. [References: 2]
机译:研究了在450-470℃下熔融15分钟的PbBr2-PbCl2-PbF2-PbO-P2O5体系中某些玻璃熔融过程中的成分变化。结果表明,批料组成与所分析的组成之间存在显着差异。大量的P,Br,Pb和Cl以PbBr2,PbCl2和P2O5的形式损失掉。 O的含量受两个因素影响。 NH4H2PO4的不完全分解或大气中P2O5与H2O之间的反应增加了O的含量,而P2O5的挥发降低了O的含量。(C)2001 Elsevier Science B.V.保留所有权利。 [参考:2]

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号