Fe-MCM-41 from Coal-Series Kaolin as Catalysts for the Selective Catalytic Reduction of NO with Ammonia

机译:煤系高岭土中的Fe-MCM-41用作氨选择性催化还原NO的催化剂

获取原文
获取原文并翻译 | 示例
   

获取外文期刊封面封底 >>

       

摘要

Fe-MCM-41, one kind of high-ordered mesoporous materials catalysts, with molar ratio of Fe/Si = 0.01-0.1, was synthesized by hydrothermal method from coal-series kaolin. Fe-MCM-41 catalysts were characterized by Fourier transform infrared spectroscopy, high resolution transmission electron microscopy, N_2 adsorption-desorption, x-ray photoelectron spectroscopy, and UV-vis spectroscopy. The results clearly indicated that: (1) all the samples exhibited typical hexagonal arrangement of mesoporous structure; (2) the incorporation of tiny amount of Fe~(3+) onto the surface and pore channel of MCM-41 mesoporous materials could efficiently promote the deNO_x activity of these catalysts. Moreover, the Fe-MCM-41 mesoporous materials were evaluated in the selective catalytic reduction of NO with NH_3. The results showed that Fe-MCM-41 catalyst with Fe/Si = 0.05 showed the highest catalytic activity at 350℃, a gas hourly space velocity of 5000 h~(-1), n(NH_3)(NO) = 1.1, and O_2% = 2.5%.
机译:以煤系高岭土为原料,通过水热法合成了Fe / Si摩尔比为0.01-0.1的一种高阶介孔材料催化剂Fe-MCM-41。 Fe-MCM-41催化剂通过傅里叶变换红外光谱,高分辨率透射电子显微镜,N_2吸附-解吸,x射线光电子能谱和紫外可见光谱进行了表征。结果清楚地表明:(1)所有样品均表现出典型的中孔结构六边形排列; (2)在MCM-41介孔材料的表面和孔道中掺入少量Fe〜(3+)可以有效地提高这些催化剂的deNO_x活性。此外,对Fe-MCM-41介孔材料进行了NH_3选择性催化还原NO的评价。结果表明,Fe / Si = 0.05的Fe-MCM-41催化剂在350℃时具有最高的催化活性,气体时空速为5000 h〜(-1),n(NH_3)/ n(NO)= 1.1 ,而O_2%= 2.5%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号