Structure and oil retaining capacity of gasar copper fabricated by radial solidification with a combined crystallizer

机译:组合结晶器径向凝固法制备的天然气铜的结构和持油能力

获取原文
获取原文并翻译 | 示例
       

摘要

Porous copper with elongated pores was fabricated by a radial solidification method. The process was carried out in a combined crystallizer under high pressure of a mixture of hydrogen and argon. Pore size, pore length, pore density and porosity of the porous copper were characterized. Furthermore, the oil retaining capacity including oil content and oil efficiency was also evaluated. It is found that porous copper solidified with water-circulated chiller through a thick graphite jacket possesses a gradient structure with increasing pore size, and thus pore density decreases. Also pore length and pore aspect ratio decrease from lateral inwardly, while its porosity is almost uniform. The results show that the porous copper with radial pores has a good oil retaining capacity.
机译:通过径向凝固法制备具有细长孔的多孔铜。该方法在高压和氢气和氩气的混合物中在联合结晶器中进行。表征了多孔铜的孔尺寸,孔长度,孔密度和孔隙率。此外,还评价了含油量和含油率的含油量。发现通过水循环冷却器通过厚的石墨套固化的多孔铜具有随着孔尺寸增加的梯度结构,因此孔密度降低。孔隙长度和孔隙纵横比也从侧面向内减小,而其孔隙率几乎均匀。结果表明,具有径向孔的多孔铜具有良好的保油能力。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号