Introduction The use of root canal filling materials with antibacterial activity could be considered beneficial to reduce any remaining microorganisms and prevent recurrent infection. The aim of this study was to evaluate the physical properties of AH Plus (Dentsply DeTrey, Konstanz, Germany) alone and mixed with 1% or 2% chlorhexidine (CHX); 0.1%, 0.2%, 0.3%, and 0.5% of cetrimide (CTR); and combinations of both. Methods Setting time, flow, solubility, and radiopacity of AH Plus and modified AH Plus were evaluated following the American National Standards Institute/American Dental Association's requirements (ANSI/ADA Specification No. 57/2000). Five samples of each material were tested for each property. The hypothesis of equality among groups was rejected by an analysis of variance test, and then a post hoc Tukey test was performed. Results AH Plus and modified AH Plus gave values that are within the required standards. Overall, results indicate that CTR increased setting time, but CHX alone and CHX + CTR reduced it. CHX increased the flow, whereas CTR reduced it, and their combinations gave intermediate values comparable with those of AH Plus. Concerning solubility, the weight loss in all samples was under the 3% limit set by the ANSI/ADA. In comparison with AH Plus alone, radiopacity gave slightly lower values with CHX, higher values with CTR, and similar values with combinations. Conclusions The addition of CHX, CTR, and combinations of both to AH Plus did not alter the physical properties specified by ANSI/ADA requirements.
机译:引言使用具有抗菌活性的根管充填材料被认为有利于减少任何残留的微生物并防止复发感染。本研究的目的是单独评估AH Plus(Dentsply DeTrey,德国康斯坦茨)的物理性能,并与1%或2%的洗必太(CHX)混合使用; 0.1%,0.2%,0.3%和0.5%的塞米特胺(CTR);以及两者的组合。方法按照美国国家标准协会/美国牙科协会的要求(ANSI / ADA规范第57/2000号)评估AH Plus和改性AH Plus的凝固时间,流量,溶解度和射线不透性。针对每种特性测试了每种材料的五个样本。组间平等的假设被方差检验分析所拒绝,然后进行了事后Tukey检验。结果AH Plus和改良版AH Plus给出的值均在所需标准之内。总体而言,结果表明CTR增加了凝固时间,但单独使用CHX和CHX + CTR减少了凝固时间。 CHX增加了流量,而CTR减少了流量,它们的组合提供的中间值与AH Plus相当。关于溶解度,所有样品的重量损失均低于ANSI / ADA设定的3%极限。与单独使用AH Plus相比,不透射线的CHX值略低,CTR的值较高,组合时的不透射率相似。结论在AH Plus中添加CHX,CTR以及两者的组合并不会改变ANSI / ADA要求指定的物理特性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号