The conditions to obtain metal microanostructures by templated electrodeposition using bicontinuous microemulsions have been proposed. For this, different microemulsions have been tested to discover, analyze and generalize the conditions that must fulfill in order to act as a template for metal electrodeposition. Bicontinuous microemulsions were selected to provide enough conductivity to permit the process at significant velocity. Using the cobalt deposition process from a single bath in the aqueous component of the microemulsion as a test, the relation between the nature of the microemulsions and the template capacity in the electrodeposition process has been deduced. Depending on the characteristics of each selected microemulsion, either continuous or nanostructured deposits (porous films or particles of 20-50 nm) were obtained. The conditions for which the microemulsions act as templates in the electrodeposition are: (1) immiscibility of oil and aqueous solution components, (2) low dielectric constant of the oil to favor the non-dissolution of the electroactive species, (3) the use of a surfactant that avoids the solubilization of electroactive species. Also, the possibility of using an electrodeposition method to characterize the structure of some microemulsions has been demonstrated.
机译:已经提出了使用双连续微乳液通过模板电沉积获得金属微/纳米结构的条件。为此,已经测试了不同的微乳状液以发现,分析和归纳为金属电镀的模板所必须满足的条件。选择双连续微乳液以提供足够的电导率以允许该方法以显着的速度进行。使用在微乳液的水性组分中一次浴中的钴沉积过程作为测试,已经推导了微乳液的性质与电沉积过程中模板容量之间的关系。取决于每种选择的微乳液的特性,获得了连续的或纳米结构的沉积物(多孔膜或20-50 nm的颗粒)。微乳液在电沉积中充当模板的条件是:(1)油与水溶液成分的不溶混性,(2)油的介电常数低,有利于电活性物质的不溶解,(3)使用避免电活性物质溶解的表面活性剂。另外,已经证明了使用电沉积方法表征某些微乳液的结构的可能性。

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号