Heteropolyanions (HPAs) of the Keggin type have been successfully applied as redox components in heterogeneous Wacker catalysts. The catalysts consist of a silica support covered with a layer of HPA of the series H3+nPVnMo12-nO40 On which a submonolayer of palladium sulfate is deposited. The initial butanone yield in the oxidation of 1-butene at 343 K is approximately 0.10 g butanone per gram of catalyst per hour. The steady-state activity is, however, a factor of 10 lower due to the slow reoxidation of reduced HPA. The rate of reoxidation and hence the steady-state activity increases with increasing number (n) of vanadium atoms per Keggin unit and when the protons of the HPA are replaced by Cu2+ Or by Ni2+. Even higher activity is obtained with palladium salts of heteropolyacids. In these palladium salts the palladium reaction centre and the redox component are combined in one complex. The butanone selectivity of the catalysts with n > 0 is high, viz. >95%, and increases with increasing values of n to more than 98%. The butanone selectivity also increases when the protons are exchanged for metal cations, such as Cu2+, Ni2+, Pd2+, or Cs+. The stability of the Keggin units under reaction conditions is high. Under Wacker oxidation conditions the HPAs are partly reduced, but DRIFT and ESR spectroscopy and TPR analysis of used catalysts show that the Keggin structure remains intact. Reoxidation of the reduced HPAs is, however, slow under reaction conditions. (C) 1995 Academic Press, Inc. [References: 34]
机译:Keggin类型的杂多阴离子(HPA)已成功地用作非均相Wacker催化剂中的氧化还原组分。催化剂由覆盖有H3 + nPVnMo12-nO40系列HPA层的二氧化硅载体组成,在其上沉积了一层亚硫酸钯亚层。在343 K下氧化1-丁烯的初始丁酮产率约为每克催化剂每小时0.10 g丁酮。但是,由于还原型HPA的缓慢再氧化,稳态活性降低了10倍。随着每个Keggin单元中钒原子数(n)的增加以及HPA的质子被Cu2 +或Ni2 +替代,再氧化的速率以及因此的稳态活性都会增加。用杂多酸的钯盐可获得更高的活性。在这些钯盐中,钯反应中心和氧化还原组分结合在一个复合物中。 n> 0的催化剂的丁酮选择性高,即。 > 95%,并且随着n值的增加而增加到98%以上。当质子交换金属阳离子(例如Cu2 +,Ni2 +,Pd2 +或Cs +)时,丁酮选择性也会增加。 Keggin单元在反应条件下的稳定性高。在Wacker氧化条件下,HPA会部分还原,但是DRIFT和ESR光谱以及使用过的催化剂的TPR分析表明Keggin结构保持完整。然而,在反应条件下还原的HPA的再氧化缓慢。 (C)1995 Academic Press,Inc. [参考:34]

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号