首页> 外文期刊>Journal of Adhesion Science and Technology: The International Journal of Theoredtical and Basic Aspects of Adhesion Science and Its Applications in All Areas of Technology >Effects of cavity disinfectants on bond strength of an etch-and-rinse adhesive to water- or ethanol-saturated sound and caries-affected dentin
【24h】

Effects of cavity disinfectants on bond strength of an etch-and-rinse adhesive to water- or ethanol-saturated sound and caries-affected dentin

机译:空腔消毒剂对浸蚀和漂洗粘合剂对水或乙醇饱和的声音和龋齿影响的牙本质的粘合强度的影响

获取原文
获取原文并翻译 | 示例

摘要

Objective: To evaluate the effect of cavity disinfectants on the immediate microtensile bond strength (TBS) of an etch-and-rinse adhesive to water- and ethanol-saturated sound and caries-affected dentin (CAD). Material and Methods: Thirty-six human molars were sectioned to expose 1/3 of the mid-coronal dentin surface. Sound (n=18) and CAD (n=18) specimens were divided into six groups each (n=3): one positive control (sound), one negative control (CAD), and five experimental groups each. In the control group, dentin surfaces were bonded using an etch-and-rinse adhesive with a traditional water-wet bonding technique. In the experimental groups, ozone was applied before etching and chlorhexidine after etching. In the ethanol-wet bonding groups, acid-etched dentin surfaces were treated with ethanol. Following adhesive application and composite buildups, bonded specimens were sectioned to form sticks. Failure modes were analyzed using a stereomicroscope. Results: The water-wet bonded sound control group yielded the highest TBS among all groups (p<0.001). The lowest TBS values were observed in the ozone groups (p<0.05). The ethanol-wet bonded CAD group exhibited a higher TBS than the water-wet bonded negative controls. Although compared to the positive control, chlorhexidine decreased the TBS (p<0.05), an increase with no significant difference was observed in the negative control (p>0.05). Conclusions: The TBS values of CAD were lower than those of sound dentin. Ethanol-wet bonding improved the TBS of CAD. Ozone application reduced the TBS in both sound and CAD; chlorhexidine improved the immediate TBS after etching in CAD.
机译:目的:评估腔体消毒剂对浸蚀和漂洗的粘合剂对水和乙醇饱和的,受龋齿影响的牙本质(CAD)的即时微拉伸粘合强度(TBS)的影响。材料和方法:将36颗人类磨牙切成薄片以暴露冠状中部牙本质表面的1/3。声音(n = 18)和CAD(n = 18)标本分别分为六组(n = 3):一个阳性对照(声音),一个阴性对照(CAD)和五个实验组。在对照组中,牙本质表面使用蚀刻和漂洗粘合剂通过传统的水湿粘合技术粘合。在实验组中,在蚀刻前施加臭氧,在蚀刻后施加洗必太。在乙醇湿键合基团中,用乙醇处理酸蚀过的牙本质表面。在施加粘合剂和复合物堆积之后,将粘合的样品切成棒状。使用立体显微镜分析失效模式。结果:在所有组中,水湿粘结声对照组的TBS最高(p <0.001)。在臭氧组中观察到最低的TBS值(p <0.05)。乙醇湿键合CAD组显示出比水湿键合阴性对照更高的TBS。尽管与阳性对照相比,洗必泰降低了TBS(p <0.05),但在阴性对照中未观察到明显的升高(p> 0.05)。结论:CAD的TBS值低于声音牙本质的TBS值。乙醇湿粘合改善了CAD的TBS。臭氧的使用降低了声音和CAD的TBS。氯己定在CAD中蚀刻后改善了即时TBS。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号