Scaffolding is an essential issue in tissue engineering and scaffolds should answer certain essential criteria: biocompatibility, high porosity, and important pore interconnectivity to facilitate cell migration and fluid diffusion. In this work, a modified solvent casting-particulate leaching out method is presented to produce scaffolds with spherical and interconnected pores. Sugar particles (200-300 microm and 300-500 microm) were poured through a horizontal Meker burner flame and collected below the flame. While crossing the high temperature zone, the particles melted and adopted a spherical shape. Spherical particles were compressed in plastic mold. Then, poly-L-lactic acid solution was cast in the sugar assembly. After solvent evaporation, the sugar was removed by immersing the structure into distilled water for 3 days. The obtained scaffolds presented highly spherical interconnected pores, with interconnection pathways from 10 to 100 mum. Pore interconnection was obtained without any additional step. Compression tests were carried out to evaluate the scaffold mechanical performances. Moreover, rabbit bone marrow mesenchymal stem cells were found to adhere and to proliferate in vitro in the scaffold over 21 days. This technique produced scaffold with highly spherical and interconnected pores without the use of additional organic solvents to leach out the porogen.
机译:支架是组织工程中的一个基本问题,支架应满足某些基本标准:生物相容性,高孔隙率和重要的孔互连性,以促进细胞迁移和流体扩散。在这项工作中,提出了一种改进的溶剂浇铸-颗粒浸出方法,以生产具有球形和互连孔的支架。将糖颗粒(200-300微米和300-500微米)倒入水平的Meker燃烧器火焰中,并在火焰下方收集。在穿过高温区时,颗粒熔化并呈球形。在塑料模具中压缩球形颗粒。然后,将聚-L-乳酸溶液浇铸在糖组件中。溶剂蒸发后,将结构浸入蒸馏水中3天以除去糖。所获得的支架呈现出高度球形的互连孔,具有从10到100μm的互连路径。无需任何其他步骤即可获得孔互连。进行压缩测试以评估支架的机械性能。此外,发现兔骨髓间充质干细胞在支架中在21天之内粘附并在体外增殖。该技术生产的支架具有高度球形和相互连接的孔,而无需使用其他有机溶剂来浸出致孔剂。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号