Comparison of plasma-sprayed hydroxyapatite coatings and hydroxyapatite/tricalcium phosphate composite coatings: In vivo study

机译:等离子体喷涂羟基磷灰石涂层与羟基磷灰石/磷酸三钙复合涂层的比较:体内研究

获取原文
获取原文并翻译 | 示例

摘要

This study aimed to compare biological properties, including osteoconduction, osseointegration, and shear strength, between plasma-sprayed hydroxyapatite (HA) and HA/tricalcium phosphate (TCP) coatings, using a transcortical implant model in the femora of canines. After 3 and 12 weeks of implantation, the implants with surrounding bone were assessed histologically in undecalcified sections in backscattered electron images (BFIs) under a scanning electron microscope (SEM). After short-term (3 week) follow-up, both coatings conducted new bone formation and revealed direct bone-to-coating contact. The HA/TCP coating could not enhance early host-to-coating responses. At 12 weeks, serious dissolution of the HA/TCP coatings evidently occurred. By the new bone healing index (NBHI) and apposition index (Al), we found no significant difference between HA/TCP-coated implants and HA-coated implants throughout all implant periods. At 12 weeks of implantation, some particles dissociated from the HA/TCP coating were found within the remodeling canal. After push-out measurements, the shear strength and failure mode of HA/TCP-coated implants were similar to those of HA-coated implants, and no statistical differences were found between either coating. Consequently, this study indicates that HA/TCP coatings have excellent biological response and may be considered suitable bioactive ceramic coatings for short-term clinical use.
机译:这项研究旨在使用经皮皮质植入的犬股骨模型比较血浆喷涂的羟基磷灰石(HA)和HA /磷酸三钙(TCP)涂层之间的生物学特性,包括骨传导,骨整合和剪切强度。植入3周和12周后,在扫描电子显微镜(SEM)的背散射电子图像(BFI)中对未脱钙的切片进行组织学评估。短期(3周)随访后,两种涂层均进行了新的骨形成,并显示出直接的骨与涂层接触。 HA / TCP涂层不能增强宿主对涂层的早期反应。在第12周,明显发生了HA / TCP涂层的严重溶解。通过新的骨愈合指数(NBHI)和并置指数(A1),我们发现在整个植入期间,HA / TCP涂层植入物与HA涂层植入物之间没有显着差异。植入12周后,在重塑管内发现了一些从HA / TCP涂层上解离的颗粒。推出测试后,HA / TCP涂层植入物的剪切强度和破坏模式与HA涂层植入物的相似,并且在两种涂层之间均未发现统计学差异。因此,这项研究表明,HA / TCP涂层具有出色的生物学响应,可以被认为是适合短期临床使用的生物活性陶瓷涂层。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号