Poly(thylene-2,6-naphthalenedicarboxylate) (PEN) has been prepared from commercial dimethyl-2,6-naphthalenedicarboxylate (DM-2,6-NDC) and ethylene glycol (EG) according to the well-known transesterification/polycondensation route. PEN fibers, intended for industrial yarn applications, were obtained by melt spinning and drawing high molecular weight PEN. The properties of these yarns were measured in detail and compared with those of PET industrial yarns. The development of molecular orientation in the spinline is more pronounced for PEN than for PET. Because the yield stress is lower, PEN yarns can more easily be drawn. Breaking tenacities of PEN yarns are comparable with those of PET yarns, but the modulus is much higher and the thermal shrinkage is lower. Therefore, PEN yarns have a better dimensional stability than PET yarns. In addition, it was demonstrated that the thermal resistance of PEN yarns is better. (C) 1995 John Wiley and Sons, Inc. [References: 24]
机译:聚(2,6-萘二甲酸二亚乙酯)(PEN)是根据众所周知的酯交换/缩聚路线由市售2,6-萘二甲酸二甲酯(DM-2,6-NDC)和乙二醇(EG)制备的。通过熔融纺丝和拉伸高分子量PEN获得用于工业纱线的PEN纤维。对这些纱线的性能进行了详细测量,并与PET工业纱线进行了比较。 PEN比PET中纺丝线中分子取向的发展更为明显。由于屈服应力较低,因此可以更轻松地拉伸PEN纱线。 PEN纱线的断裂强度与PET纱线的断裂强度相当,但模量更高,热收缩率更低。因此,PEN纱比PET纱具有更好的尺寸稳定性。另外,证明了PEN纱线的耐热性更好。 (C)1995 John Wiley and Sons,Inc. [参考:24]

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号