Afailure was detected during the shutdown of an HF alkylation unit,when a leak was discovered after chemical cleaning of the pipe.The perforation occurred at a weld joining a 90 deg elbow with a straight pipe section.The failed section was removed for replacement.Internal visual inspection revealed preferential corrosion at the weld.
机译:HF烷基化装置关闭期间发生化学故障,当管道化学清洗后发现泄漏时,在连接90度弯头与直管段的焊缝处发生穿孔,将故障段移除以进行更换。目视检查发现焊缝处优先腐蚀。