Recovery of molybdenum and vanadium with high purity from sulfuric acid leach solution of spent hydrodesulfurization catalysts by ion exchange

机译:通过离子交换从废加氢脱硫催化剂的硫酸浸出溶液中回收高纯度的钼和钒

获取原文
获取原文并翻译 | 示例
           

摘要

Valuable metals, such as Mo, V, Co and Ni together with base metals (Fe and Al) are present in the sulfuric acid leaching solutions of spent hydrodesulfurization catalysts. In order to develop a process to recover pure Mo and V from the solution, batch and continuous ion exchange experiments with strong anionic resin (AGl-x8) have been performed by employing a synthetic sulfuric acid solution. Batch experimental results indicated that the separation of molybdenum and vanadium from the solution with AGl-x8 was possible by adjusting the pH of the solution to 0.5 and 1.6, respectively. Column experimental results verified the complete separation and recovery of molybdenum and vanadium from the solution at the specified pH conditions. Molybdenum and vanadium in the loaded resin was eluted by using NaOH solution. The purity of Mo and V solution after elution was found to be higher than 99%. After elution, AG1 -x8 was successfully regenerated by converting its form from hydroxide to chloride by using NaCl solution.
机译:废加氢脱硫催化剂的硫酸浸出溶液中存在贵重金属,例如Mo,V,Co和Ni,以及贱金属(Fe和Al)。为了开发一种从溶液中回收纯Mo和V的方法,已经通过采用合成硫酸溶液进行了强阴离子树脂(AG1-x8)的分批和连续离子交换实验。批量实验结果表明,通过将溶液的pH值分别调节到0.5和1.6,可以用AG1-x8从溶液中分离钼和钒。色谱柱实验结果证实了在指定的pH条件下从溶液中完全分离和回收了钼和钒。使用NaOH溶液洗脱负载树脂中的钼和钒。发现洗脱后的Mo和V溶液的纯度高于99%。洗脱后,使用NaCl溶液将AG1-x8的形式从氢氧化物转化为氯化物,从而成功地再生了AG1-x8。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号