摘要

A novel staged leaching process has been reported in this paper to extract Ag and Au and their associated valuable metals including Cu, Zn and Pb from a complex polymetallic sulfide concentrate with high Fe, As and Sb. The Ag in this concentrate primarily occurs in tetrahedrite, and Au is also partly encapsulated by sulfide minerals. At first, 98.2% of Cu and 95.8% of Zn were extracted by oxygen pressure leaching with sulfuric acid, and then 95.7% of Pb was extracted by silicofluoric add leaching. After these two stages of leaching, the dissolution for both Ag and Au was negligible, and the overall leaching of Fe, As and Sb reached 91.6%, 71.1% and 48.8%, respectively. Ag was concentrated in silicofluoric acid leach residue primarily as Ag2S while Au became more accessible to lixiviant Afterwards, 96.8% of Ag and 94.7% of Au in the residue were extracted by two-step countercurrent nickel catalyzed thiosulfate leaching. The silver in the final residue mainly occurred in antimonate and arsenate, and most of the remaining gold was encapsulated by pyrite and these oxysalts. (C) 2015 Published by Elsevier B.V.
机译:本文报道了一种新颖的分步浸出工艺,用于从具有高Fe,As和Sb的复杂多金属硫化物精矿中提取Ag和Au及其相关有价金属,包括Cu,Zn和Pb。该精矿中的Ag主要存在于四面体中,Au也被硫化物矿物部分包封。首先,通过硫酸的氧压浸提法提取了98.2%的Cu和95.8%的Zn,然后通过硅氟添加浸提法提取了95.7%的Pb。经过这两个浸出阶段,Ag和Au的溶出量可以忽略不计,Fe,As和Sb的总浸出率分别达到91.6%,71.1%和48.8%。 Ag主要以Ag2S的形式富集在氟硅酸浸出渣中,而Au则更容易浸出。随后,通过两步逆流镍催化的硫代硫酸盐浸提法,将残留物中的96.8%Ag和94.7%Au萃取出来。最终残留物中的银主要存在于锑酸盐和砷酸盐中,剩余的大部分金被黄铁矿和这些含氧盐包裹。 (C)2015由Elsevier B.V.发布

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号