Separation of nickel(II), cobalt(II) and lanthanides from spent Ni-MH batteries by hydrochloric acid leaching, solvent extraction and precipitation

机译:通过盐酸浸提,溶剂萃取和沉淀分离镍氢电池中的镍,钴和镧系元素

获取原文
获取原文并翻译 | 示例
           

摘要

The separation of nickel(II), cobalt(II) and lanthanides from chloride leach liquors of spent nickel-metal hydride (Ni-MH) batteries is described. After leaching in 12 mol L~(-1) HC1, the traces of iron(III) and zinc(II) were extracted in a single stage with pure TBP (25 °C, A/O ratio = 1 v/v). Cobalt was extracted (93.6%) in two stages with Alamine 336 (10% vol. in kerosene, 25 °C A/O = 1 v/v, free acidity=4.3 mol L~(-1)). More than 98% of the lanthanides present in the raffinate were recovered through one of the following routes: (i) extraction with PC88A (20 vol.% in kerosene, 25 ℃, A/O = l v/v, one stage, pH 1); (ii) precipitation as oxalates at pH 0.5. Nickel(II) was precipitated (>99%) as oxalate at pH 2. Metals separation in acidic medium avoids partial or total neutralization of the leachate and reduces the amount (and salinity) of the wastewater generated in the separation processes.
机译:描述了从废镍金属氢化物(Ni-MH)电池的氯化物浸出液中分离镍(II),钴(II)和镧系元素。在12 mol L〜(-1)HCl中浸提后,用纯TBP(25°C,A / O比= 1 v / v)在单一阶段中萃取痕量的铁(III)和锌(II)。用Alamine 336(10%的煤油体积,25°C A / O = 1 v / v,游离酸度= 4.3 mol L〜(-1))分两步萃取钴(93.6%)。通过以下途径之一回收了萃余液中存在的98%以上的镧系元素:(i)用PC88A萃取(20体积%的煤油,25℃,A / O = lv / v,一级,pH 1 ); (ii)在pH 0.5沉淀为草酸盐。在pH 2时,草酸镍(II)沉淀(> 99%)。在酸性介质中进行金属分离可避免部分或全部中和渗滤液,并减少了分离过程中产生的废水量(和盐度)。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号