This paper presents a new method of recycling aluminum and iron in boiler slag derived from plants that use coal as fuel. The new method integrates efficient extraction and reuse of the leached pellets together. An elemental analysis of aqueous solutions leached by sulfuric acid was determined by EDTA-Na2-ZnCl2 titra-tion method. The components and microstructures of the samples were examined by means of XRF, XRD and SEM. An aluminum extraction efficiency of 86.50% was achieved when the sintered pellets were leached using 4 mol - L ' H_2SO4 at solid/ liquid [m(g)/K(mL)] ratio of 1 : 5 at 80 deg C for 24 h. An iron extraction efficiency of 94.60% was achieved in the same conditions for the maximum extraction efficiency of Al. The extraction efficiencies of Al and Fe increased with an increase in temperature, leaching time and acidity. The concentration of alumina and iron hydroxide in the final product was determined to be 99.12% and 92.20% respectively. This product of alumina would be used directly for the production of metallic aluminum.
机译:本文提出了一种回收利用煤为燃料的工厂产生的锅炉炉渣中铝和铁的新方法。新方法将沥滤颗粒的有效提取和再利用整合在一起。用EDTA-Na2-ZnCl2滴定法测定硫酸浸出的水溶液的元素分析。用XRF,XRD和SEM检查样品的成分和微观结构。当使用4 mol-L'H_2SO4以固/液[m(g)/ K(mL)]比为1:5的比例在80℃下浸提24小时后,烧结颗粒的铝提取效率达到86.50%。在相同的条件下,Al的最大铁提取效率达到94.60%。随着温度,浸出时间和酸度的增加,铝和铁的萃取效率也随之提高。最终产品中氧化铝和氢氧化铁的浓度分别确定为99.12%和92.20%。该氧化铝产品将直接用于生产金属铝。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号