Total number of heats taken in tundish refractory working linings (MgO-based) varies with three steel grades produced in the Long Product Complex at Tata Steel. The duration of the sequence heats (of 60-70 min) for low-C, med-C and high-C steel grades made at billet caster are 14-16, 16-18 and 22-24 h respectively. These differences are due to different rates in erosion and corrosion of the three types of tundish slags arising in three different steel grades and different liquidus temperatures of three steel grades. The tundish slags have different chemical compositions, liquidus temperatures and viscosity. An attempt has been made in the present work to understand the wear mechanisms of MgO-based refractory linings by different tundish slags in the three steel grades. Chemical analysis, optical and scanning electron microscopy (SEM), and energy dispersive spectroscopy (EDS) have been used to characterize the slag infiltrated MgO-based tundish lining samples collected from the plant. The present work has been undertaken to find out the wear mechanism by different tundish slags, take corrective measures with regard to slag chemistry and MgO lining material to minimize the erosion and corrosion, and enhance the continuous casting durations.
机译:塔塔钢铁长材生产厂生产的中间包耐火材料衬里(基于MgO)的总热量因三种钢种而异。在方坯连铸机上生产的低碳,中碳和高碳钢的顺序加热时间(60-70分钟)分别为14-16、16-18和22-24小时。这些差异是由于三种不同钢种产生的三种中间包渣的腐蚀和腐蚀速率不同以及三种钢种的液相线温度不同所致。中间包渣具有不同的化学组成,液相线温度和粘度。在目前的工作中,人们试图通过三种钢种的不同中间包渣了解MgO基耐火衬里的磨损机理。化学分析,光学和扫描电子显微镜(SEM)以及能量色散光谱(EDS)已用于表征从工厂收集的炉渣浸润的基于MgO的中间包衬里样品。目前的工作是为了找出不同中间包渣的磨损机理,对炉渣化学成分和MgO衬里材料采取纠正措施,以最大程度地减少腐蚀和腐蚀,并延长连铸时间。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号