Characterisation of thermal properties of oxide, reduced and sulphided forms of alumina supported Co(Ni)-Mo(W) catalysts prepared by co-precipitation

机译:共沉淀制备的氧化铝,负载型Co(Ni)-Mo(W)催化剂的氧化物,还原形式和硫化形式的热学性质

获取原文
获取原文并翻译 | 示例
   

获取外文期刊封面封底 >>

       

摘要

This study deals with alumina supported Co(Ni)-Mo(W) catalysts prepared in one step by the co-precipitation method. Results of temperature-programmed reduction (TPR) of oxide forms of the catalysts, and differential thermal analysis (DTA) and thermal gravimetry (TG) of the oxide, reduced and simultaneously reduced and sulphided forms of the catalysts are presented. Reduction of the catalysts has been found to begin already at about 150 degreesC. It has been established that at 400 degreesC the CoMo catalyst practically does not reveal any mass loss after 30 min reduction with hydrogen, while the NiMo catalyst shows a large mass loss after 60 min reduction, continuing with time. The catalyst NiW also shows a significant mass loss already after 10 min reduction with hydrogen, and this mass loss continues to occur as the time of reduction increases. (C) 2001 Elsevier Science BN. All rights reserved. [References: 5]
机译:这项研究涉及通过共沉淀法一步制备的氧化铝负载的Co(Ni)-Mo(W)催化剂。给出了催化剂的氧化物形式的程序升温还原(TPR),氧化物的差示热分析(DTA)和热重分析(TG),还原,同时还原和硫化形式的催化剂的结果。已经发现催化剂的还原已经在约150℃开始。已经确定,在400℃下,用氢气还原30分钟后,CoMo催化剂实际上不显示任何质量损失,而在60分钟还原后,NiMo催化剂显示出较大的质量损失,并随时间持续。催化剂NiW在用氢气还原10分钟后也已经显示出明显的质量损失,并且这种质量损失随着还原时间的增加而继续发生。 (C)2001 Elsevier Science BN。版权所有。 [参考:5]

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号