In this work, calcium-modified lead titanate (Pb1-xCax)TiO3 (PCT) precursor solutions with different amounts of Ca2+ substituting Pb2+ (x = 0.24 and 0.50) have been prepared for the first time by an entirely aqueous solution-gel route. The use of water as a nonhazardous and inexpensive solvent, together with the easy handling of the technique (no inert atmosphere is required), are the major advantages of this method. A stable citrato-peroxo complex of Ti(IV) was synthesized first and subsequently combined with the Pb2+ and Ca2+ reagents (citrates) in the desired molar ratio to obtain the aqueous precursor solutions. The stability of these solutions with time is slightly influenced by the amount of Ca2+ introduced in the PCT system. Gels were obtained from these solutions and subjected to thermogravimetric analysis coupled on-line to Fourier transform infrared (TGA-FTIR) and mass spectroscopy (TGA-MS) techniques. To prepare thin films, we had to improve the hydrophilicity of the Pt/TiOx/SiO2/Si substrates and hence their wetting by the aqueous solutions using a wet chemical treatment of cleaning. Crystallization of the films was carried out by rapid thermal processing (RTP) in air at 650 degrees C. Films with a single perovskite phase and a homogeneous microstructure were thus obtained, as deduced by X-ray diffraction (XRD) and scanning electron microscopy (SEM). The ability of this solution method to obtain PCT films with ferroelectric and dielectric responses is also demonstrated in the present work.
机译:在这项工作中,通过完全水溶液-凝胶途径首次制备了钙改性的钛酸铅(Pb1-xCax)TiO3(PCT),其中Ca2 +取代Pb2 +的量不同(x = 0.24和0.50)。使用水作为一种无害且廉价的溶剂,以及该技术易于处理(不需要惰性气氛),是该方法的主要优点。首先合成稳定的Ti(IV)的citrato-peroxo配合物,然后以所需的摩尔比与Pb2 +和Ca2 +试剂(柠檬酸盐)混合,以获得水性前体溶液。这些溶液随时间的稳定性受PCT系统中引入的Ca2 +量的影响很小。从这些溶液中获得凝胶,并进行热重分析,并在线耦合至傅立叶变换红外(TGA-FTIR)和质谱(TGA-MS)技术。为了制备薄膜,我们必须提高Pt / TiOx / SiO2 / Si基材的亲水性,并因此通过使用湿化学清洁法处理水溶液来润湿它们。薄膜的结晶化是通过在650摄氏度的空气中通过快速热处理(RTP)进行的。因此,通过X射线衍射(XRD)和扫描电子显微镜推论得出了具有单一钙钛矿相和均匀微观结构的薄膜( SEM)。在本工作中也证明了该溶液方法获得具有铁电和介电响应的PCT膜的能力。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号