Effect of phosphoric acid etching and self-etching primer application methods on dentinal shear bond strength.

机译:磷酸蚀刻和自蚀刻底漆施加方法对牙列剪切粘结强度的影响。

获取原文
获取原文并翻译 | 示例
获取外文期刊封面目录资料

摘要

PURPOSE: To evaluate acid-etching effects prior to the application of self-etching primer and the effect of different primer application techniques on dentin shear bond strength (SBS). MATERIALS AND METHODS: Forty human third molar cervical regions were used in this study. The teeth were randomly divided into four groups (n=10) of different tooth surface conditions: group A: Clearfil Protect Primer applied gently (inactive) + Clearfil Protect Bond; group B: 38% phosphoric acid for 15 s, rinsed 15 s, and dried 15 s + Clearfil Protect Primer applied gently (inactive) + Clearfil Protect Bond; group C: Clearfil Protect Primer applied with agitation by microapplicator brush (active) + Clearfil Protect Bond; group D: 38% phosphoric acid for 15 s, rinsed 15 s, and dried 15 s + Clearfil Protect Primer applied with agitation by microapplicator brush (active) + Clearfil Protect Bond. The SBS test was performed with a universal testing machine at a crosshead speed of 1 mm/min. Data were analyzed with one-way ANOVA and Tukey HSD tests. RESULTS: The mean SBS values (MPa) and standard deviations are as follows: group A: 36.0 +/- 8.3; group B: 24.0 +/- 3.9; group C: 35.0 +/- 3.3; group D: 30.6 +/- 6.7. CONCLUSION: Acid etching decreased the SBS of the self-etching bonding system to dentin. Active primer application increased the SBS only in acid-etched groups.
机译:目的:评估在施加自蚀底漆之前的酸蚀效果,以及不同底漆施加技术对牙本质剪切粘合强度(SBS)的影响。材料与方法:本研究使用了40个人类第三磨牙宫颈区域。牙齿被随机分为四组(n = 10),它们的牙齿表面状况不同:A组:轻轻地(不使用)Clearfil Protect Primer + Clearfil Protect Bond施加; B组:38%磷酸15秒钟,漂洗15秒钟,干燥15秒钟+轻轻地(无活性)施加Clearfil Protect Primer + Clearfil Protect Bond; C组:Clearfil Protect Primer,通过微涂刷(有源)+ Clearfil Protect Bond搅拌施加; D组:38%磷酸15秒钟,漂洗15秒钟,干燥15秒钟+用微涂刷(有源)搅拌的Clearfil Protect Primer + Clearfil Protect Bond。使用通用测试机以1 mm / min的十字头速度执行SBS测试。使用单向方差分析和Tukey HSD测试分析数据。结果:平均SBS值(MPa)和标准偏差如下:A组:36.0 +/- 8.3; B组:24.0 +/- 3.9; C组:35.0 +/- 3.3; D组:30.6 +/- 6.7。结论:酸蚀降低了自蚀结合体系与牙本质的SBS。主动引物的应用仅在酸蚀基团中增加了SBS。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号